Alexandre Bigot 1862-1927 was a professor of chemistry and physics who became interested in ceramics at the Exposition Universelle of 1889 at the age of 27.

Bigot's ceramic studios in Rue des Petites Ecuries, Paris and Mer operated from 1889 to 1914 employing 150 people at its peak.

Bigot obtained a 1906 patent for making thick once-fire glazed structural ceramic pieces.

http://www.google.com/patents/US838496

Damp glaze was applied to the mold and dry gres flammé clay placed on top, or the reverse order, before applying a pressure with a hydraulic press followed by a kiln firing.

He produced the designs of many artists and architects of the French Art Nouveau movement; including: Jules Lavirotte, Hector Guimard, Louis Majorelle, Henri Sauvage, Henry van de Velde, Auguste Perret, Andre Arfidson, Anatole de Baudot and others.

He obtained a second patent in 1924 for a drying kiln.

http://www.freepatentsonline.com/1497084.pdf

Views: 111

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics


Stars
Comment by Norm Stuart on October 24, 2013 at 3:28pm

Small-scale Alexandre Bigot, dated 1900, Sitzender Bär (Sitting Bear). Appears to be a mix of the same glazes he used on his massive thick architectural pieces.

Hetjens German Ceramics Museum, Dusseldorf.


Stars
Comment by Norm Stuart on September 10, 2013 at 1:21am

The secret of making very thick structural ceramic pieces was using dry clay, damp glaze, and a hydraulic press.

The dry gres flammé clay body could not have contained raw kaolin or clay, which releases water between 850 F and 1,200 F, making such thick pieces explode.

Gres flammé was likely calcined clay, silica and a ceramic flux mixed with binders. The unglazed surface of gres flammé is very fine, revealing little presence or sand or coarse grog.

My first attempt at making Gres Flammé will be Kyanite mixed with Talc, partly due to their properties and partly because they're both grey color. Then I'll press it in a mold with whatever pressure I can devise.

http://digitalfire.com/4sight/material/kyanite_951.html

http://digitalfire.com/4sight/material/talc_1620.html

The properties of gres flammé seems to coincide with my recent interest in flameware. But using Talc as a flux may not be the best place to start, as Digitalfire states:

Talc is truly a curious material. By itself it is a refractory powder; yet in amounts of only 1-5% in stoneware or porcelain bodies it can drastically improve vitrification!

Yet cone 06-04 ceramic slips containing up to 60% talc can often be fired to cone 6 without melting or even deforming!

Notwithstanding this, other 50:50 talc:ball clay bodies will completely melt and boil at cone 6!

In glazes at middle temperature raw talc is refractory, its presence tends to create opaque and matte surfaces.  Yet if supplied as part of a frit it can create wonderfully transparent glossy glazes.

At cone 10 it is a powerful flux but also can be used in combination with calcium carbonate to create very tactile magnesia matte glazes (the MgO forms magnesium silicate crystals on cooling to give both opacity and a matte silky surface).

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by