Norm,
I think it needs to be applied pretty thin. I think the Alberta Slip you have would look more similar if very thin. I have a terrible time with glaze thickness. I have a couple that need to be thick and some very thin. I always have to do a couple of test firings with new glazes to find how it is suppose to go on.
Jeff,
No, I didn't have any problems with cracking or peeling. Went on very nicely. I also calcined part of the Alberta Slip. I just put it in a big bowl in the bisque fire. I calcine part of my EPK for my kiln wash. I have bowls I use that were chipped in bisque and never glazed. I have refired them about six times now.
Make sure and post some pics when its done. I'm going to try layering a couple of Ravenscrag recipes, but I'll have to wait until I fix my kiln. Got the relays replaced, but now I kilned one of the elements, but thats a whole nuther story! jhp
Chantay,
Did you have any problems with the dry glaze cracking or peeling or crawling in the firing? I remember seeing the recipes saying to calcine half of the slip. I didn't want to do that so I either used Ravenscrag 100%(you don't have to calcine it) or I would mix the Alberta & Ravenscrag 50/50 in the recipe. They always came out nice. I have also used Ohio slip which they say is very close to Albany slip. It worked really well also. jhp
I think we're going to buy some Alberta Slip on our next order. That's nice looking - a lot more interesting than this electrical pole insulator brown that our vintage bag of Albany Slip creates - shown here at cone 6 with the addition of 20% lithium carbonate.
.
It has the same yellow crystallization we get with Vee's Tenmoku Gold using the Digitalfire formula to make our own replacement Cornwall Stone.
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014
© 2026 Created by Andrea Wolf.
Powered by
You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!
Join Electric Mid&Hi Fired Ceramics