This is Strontium Crystal Magic+1% Silicon Carbide with Jenn's Juicy Fruit, Water Color Green, and Hanna's Fake Ash sprayed over. These are white ^5-7 Ash Stoneware from Mile Hi Ceramics.

Views: 163

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by Anthony Andersen on March 23, 2011 at 11:41pm

For ^6-6.5 firings, I used Mile Hi Aspen. Mile Hi is my local shop. Here's the blurb from their web site:

Aspen (Cone 5-7) This fine, translucent porcelain was developed as an alternative to Cone 10 firing. Aspen responds well to hand modeling or wheelwork.

http://www.milehiceramics.com/clay.htm

My only issue with that clay is you have to trim the bottom or really be careful with compression because it's much more likely to crack than any other clay I work with (including other porcelains) if the bottom is fairly thin. That being said, I've had really good results with that clay from ^5 to ^6.5 in oxidation and reduction and it's really nice to throw.

 

I expect that "The Coup" from Matt and Dave's Clays would also be good at that range. It's ^5-8. I've had good luck with their ^8-12 "Porcelain for the People" at ^8 oxidation and ^10 reduction and I plan to try "The Coup" soon.

http://www.mattanddavesclays.com/store/


Stars
Comment by Mary Jane on March 23, 2011 at 9:45pm

Thanks so much for the information.  Also, I learned from your post that Mile Hi sells clay that is 5-7 firing range.  Very good to know.  My clay says cone 5 but will go to 6 - but I hear it bloats if you go any higher than that.  5-7 would be perfect.

 

What porcelain did you use?  What is the firing range of the porcelain?  I found that the glazes from the SH workshop did look and perform (i.e. no blisters, etc) better on porcelain.  Thanks again for the info.  Cheers, MJ

Comment by Anthony Andersen on March 23, 2011 at 9:29pm
In case I wasn't clear - I used the exact recipe from the Lakeside Pottery website as the SCM base.
Comment by Anthony Andersen on March 23, 2011 at 9:27pm

There was actually a little iron in the SCM. I had a little SCMO, also with 1% SiC, so I mixed it in with the SCM. It was probably between 10% and 15% of the total. Put another way, you'd add 1/10 to 1/7 of the amount of Yellow Iron to SCM as you'd normally add for SCMO.

The Water Color Green, Jenn's Juicy Fruit, and Hanna's Fake Ash were unchanged.

 

I did have a little bit of pinholing on the stoneware so I think that may have done better a little hotter. The porcelain didn't have any problems.

 

My blog shows what the glaze looked like before firing in case you're interested...

http://anthonyandersen.blogspot.com/2011/03/sprayed-cone-6-12-scmsi...

 

Firing Schedule:

200/hr to 200

400/hr to 1900

200/hr to 2160 - hold for 1 hour

-500/hr to 1900

-125/hr to 1400

 

Here's the Orton Cones - 5, 6, 7, clockwise from bottom.


Stars
Comment by Mary Jane on March 23, 2011 at 8:44pm
Ah - forget to ask about the firing schedule.  Thanks, MJ

Stars
Comment by Mary Jane on March 23, 2011 at 8:41pm
Hello - Really like the cups.  Did you modify the recipe for strontium crystal magic other than the 1 percent silicon carbide?  The recipe i have is for cone 8 with an unusual firing schedule.  You mention that you fired this to cone 6.  Same question for Jenn's Juicy Fruit and Water Color Green and Hanna's Fake Ash.  The recipes i am using is from the Stephen Hill workshop and also shown on the lakeside Pottery website.  Any help on this is appreciated.  Great cups.  Cheers, MJ

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014