Cone 6 electric. Porcelain. Chrome tin pink with blue highlights. Matching salt and pepper shakers.

Views: 301

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by Zoophagous on January 12, 2010 at 1:17pm
I use a mid-fire porcelain.

Awaji Porcelain (SP690)
Comment by Zoophagous on January 12, 2010 at 11:29am
The blue is a drizzle of a blue glaze. I use a mid-fire (cone 6) crystal glaze with some cobalt. I prefer to use this glaze as an accent as the crystal glazes melt really well so I get some cool flows and interactions.
Comment by Zoophagous on January 11, 2010 at 9:02pm
I fired these in an older electric kiln with a kiln sitter. No controller so no schedule. Just a free cooling from cone 6.

Unless I am mistaken green would indicate that there is too much chrome. I use 0.5%.
Comment by Zoophagous on December 19, 2009 at 10:26am
Here's the recipe I use:

21 Grestely Borate
16 Neph Syn
11 EPK
20 Whiting
32 Silica

5 Tin Ox
0.2 Chrome Ox

No idea why a Chrome tin pink would be white. Maybe not enough chrome or too much tin? Be careful with the chrome though - powerful stuff. Too much and it will be brown or green. Nasty.
Comment by George Lewter on December 18, 2009 at 7:53pm
Wow, Intense red. I tried 2 chrome tin pink recipes. I think they both remained clear. Don't know what happened, but this makes me want to give it another try.

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service