Comment by Michele Hartung on September 25, 2012 at 3:32pm

Looks wonderful where you dipped it once.  I remember Steven saying that the spotted orange needed to be thin,  must be the same with this version.  Thank you for sharing this!

Comment by Sylvain Boucher on September 25, 2012 at 12:47pm

I Know it's been a while since this post, but in the case it can helps here what i found! I only did a test tile with it yet.

I dipped it once and the a second time for the corner only.

This is Jen's Juicy Fruit

Epk 10

Gerstley borate 9

Nepheline Syenite 49

Flint 12

Whiting 11

Lithium Carbonate 9

total 100

Add 

Soda Ash 10

Rutile 6

Red Iron oxide 4



Stars
Comment by Michele Hartung on July 10, 2010 at 3:23pm
Ok, thanks, Robert. I on the search for that brilliant orange. I have a feeling that it the reduction kiln that makes the difference in this case.
Comment by Robert Seele on July 10, 2010 at 8:21am
This was a pot from the SH workshop. I haven't done much trying to get the same results. Hope to in the near future.

Stars
Comment by Michele Hartung on July 10, 2010 at 8:02am
This is the spotted black look I have been trying to get back to since the SH workshop. You can see on my profile picture that I was able to get it while at the workshop, but now that I am home I am not getting the brilliant orange. Can you share any tips about mixing or using the spotted black glaze? Thanks

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014