Opulence glazes:
Autumn Frost over Black
Clay is Standard 378

Views: 107

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics


Stars
Comment by susan claysmith on December 19, 2011 at 2:23pm

Thanks a lot Sharon for sharing all of your ideas and experience with these.  Much appreciated!  I'm inspried to try making a few over the holidays.  Happy holidays ~:) Susan

Comment by Sharon Ivy on December 19, 2011 at 2:15pm
Susan, I'm replying to you on my iPad and accidentally deleted your post with the question about the knitting bowls. My apologies!
Comment by Sharon Ivy on December 19, 2011 at 2:12pm
Hi Susan. I love using knitting bowls when I knit and can only speak to what I prefer. Actually, my very favorite is a shouldered jar with a narrow opening large enough to squeeze a ball of yarn through, but not so large that the ball pops out when I tug on it. This I can place on the floor at my feet and knit away. For the bowls, I like a good thick base and I leave extra clay at the bottom so it has enough weight to stay put while I'm knitting. Yes, the inward rim is a big help I think, but I see many that are shaped more like serving bowls.

I prefer slots to holes simply because I may want to switch to a smaller bowl once my ball of yarn dwindles and the slot makes it possible to do that. I keep meaning to put little semi-circle cutouts on the rims to serve as a resting place for my needles, but I forget. Something similar to a rice bowl that has cutouts on one side and 2 small holes on the other for chopsticks. Does this all make sense?

For someone who does color work, you could make a larger bowl and have multiple slots or holes for multiple balls of yarn. I've also seen bowls with lids that serve to keep playful little cat paws away from the yarn balls. Smooth bottoms are good or you could glue felt on the bottoms. I haven't done this, but think I may start offering it if the customer wants it. I hope this helps.

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service