10" Vase w/black on the inside and persimmon over an iron red on the outside.

Views: 271

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by Steven Showalter on October 30, 2013 at 7:02am

George, I just saw this morning the recipes for discussion page with 'persimmon' on it. I had mentioned awhile back that my glaze wasn't public because the persimmon isn't from the Sankey Glaze Database. Having said that, many glazes can be made successfully a number of different ways -- so perhaps the recipe posted there works fantastic, it just isn't the recipe I use. 

Comment by George Lewter on October 29, 2013 at 8:32pm

Simply beautiful. A couple of Persimmon variations are in the Recipes for Testing Discussion. No one has verified if they are the same Persimmon that Steven Showalter or other members are using.


Stars
Comment by Michele Hartung on July 25, 2011 at 4:58pm
Steven, I agree with your testing philosophy.  I always start my throwing days with 6-8 cups for the next kiln load.  You really have this one nailed.  Beautiful and unusual and wonderful that you can replicate it.
Comment by Steven Showalter on July 24, 2011 at 8:52pm

@Michele, the persimmon glaze has some lithium in it and when it is applied over both the iron red and also the black it has a similar effect. I'm a big proponent of massive testing, and sometimes with all that testing you get lucky, and if you do enough testing you start to see trends and things become much easier to predict.

 


Stars
Comment by Michele Hartung on June 17, 2011 at 3:05pm
What do you think was the cause of the stripe of crystals on the upper part?
Comment by Steven Showalter on June 15, 2011 at 6:14pm

All my work that I put on this website is at cone 6, but I also sometimes do cone 10 reduction and I also have a wood-burning kiln I fire too. I just meant that at cone 6 you have to do a bit more work on your glazes whereas cone 10 things you can rely more on the flame. 

 


Stars
Comment by Randy McCall on June 15, 2011 at 6:08pm
So is this work at Cone 10 or Cone 6?
Comment by Steven Showalter on June 15, 2011 at 3:31pm

Iron reds do take quite a bit of work/testing at cone 6, whereas at cone 10 I don't find a whole lot of trouble with them. Its nice when you have one that works!


Stars
Comment by Randy McCall on June 15, 2011 at 1:44pm

CHT (C Harris Temoku) is probably the best iron red I have ever used. Very repeatable.

Comment by Steven Showalter on June 15, 2011 at 11:38am

Persimmon is not a 'public' glaze. When used over this particular version of iron red it produces a copper iridescence. When used by itself it is orange with some iridescence too. What is CHT?

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service