Views: 101

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics


Stars
Comment by rose maguire on June 8, 2012 at 3:12pm

Have a concept but still deciding how to achive the desired effect,will keep you posted


Stars
Comment by Jan Wallace on June 7, 2012 at 3:05pm

Its a good idea Rose and we must see the finished result. How are you going to decorate this piece?


Stars
Comment by rose maguire on June 7, 2012 at 2:58am

Its fun Jan, I throw the body of the vessel separately to the 'collar' the collar I throw baseless cut it off the wheel head and either slap/stretch and add texture (which didn’t really show up on the photo) or add texture and then do the slap/stretch, before attaching it to the body and then with the wheel at a very low speed refine the 'fit' of the neck... then add lugs etc. Love playing with this as it gives a bit more spontaneity or 'Random-ness' to the overall form.

 


Stars
Comment by Jan Wallace on June 7, 2012 at 2:12am

Hi Rose, can you please explain what you mean by composite construction? I like what you are doing here. Looks great.


Stars
Comment by rose maguire on June 6, 2012 at 6:11pm

Sneek peek of my latest  experiments with composite construction and thick runny slip

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service