I spent the past few days throwing a large amount of test tiles using 3 different cone 6 bodies to test both in cone 6 oxidation and soda. Can someone please share their cone 6 oxidation schedule for me to test both the SH glazes and my own cone 6 calcium matts and other glazes.
Stevens higher cone firing schedule is on his page, but not the cone 6. From what I have garnered reading some messages…