From John Britt
Magruder Red cone 6
Here is a really nice cone 6 Iron red. Don't have an image but trust me- it is nice!If you get an image - send it to me and I will post it.Magruder’s (Iron ) Red cone 6 oxidation44.8 Kona F-412.3 Silica18.2 Talc16.1 Bone Ash 4.3 EPK 4.3 Lithium Carbonate
2. Bentonite12.3 Synthetic Iron Oxide
I would like to try it out. Anyon…