What is your experience with ceramics in general. (Long answer encouraged)
I bought a slab roller and my Cress kiln about 15 years ago in order to make my own tiles for mosaic work. I built up knowledge through classes and a lot of self teaching...making mistakes and solving problems in less convential ways. After a few years and a bunch of successful installations I taught some classes in tile design and mosaic.

I also was involved with the building trades so many other materials and mediums were incorporated in my design work. Eventually I became more of a designer and less of a maker...until recently. I am happiest making and fill my time between design jobs reconnecting with my love for clay. I've even been experimenting with porcelain clay...I'm very humbled by it, but by working on small minimalist pieces I've improved my technical skills and have fallen in love with it.
What is your current involvement with electric fired ceramics? (long answer encouraged)
I am hoping to open an Etsy store soon (and update my website). I've been showing my work at a few local holiday gift shows and so far I'm encouraged to continue my experimentation in porcelain.
All our content is viewable by the public. Why do you want to be a member, when you can already see everything as a non-member?
I'm falling in love with porcelain clay (albeit humbled). As I continue my exploration I seem to have more questions than answers. Joining a forum like this is just what I need. Also, because I was not formally trained in ceramics I often have unconventional ways to approach my work... perhaps some of my mistakes, techniques or shortcuts would be useful to others too.
Where do you work on your ceramics projects?
home studio
Do you have your own, or participate in other ceramics Websites:
http://moxiedesign.info
How did you find this network?
search engine

Comment Wall

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

  • No comments yet!
 
 
 

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014