Dave Lyons
  • Male
  • Pittsville, WI
  • United States
Share on Facebook MySpace
  • Blog Posts
  • Discussions
  • Events
  • Groups
  • Photos (1)
  • Photo Albums
  • Videos
 

Dave Lyons's Page

Profile Information

What is your experience with ceramics in general. (Long answer encouraged)
amateur
What is your current involvement with electric fired ceramics? (long answer encouraged)
Functional stoneware and tiles,
All our content is viewable by the public. Why do you want to be a member, when you can already see everything as a non-member?
Cone 6 glazes and combinations of glazes for my own use.
Where do you work on your ceramics projects?
community center
How did you find this network?
referred by friend

Dave Lyons's Photos

  • Add Photos
  • View All

Comment Wall (4 comments)

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

At 7:26am on January 19, 2025, Ronald Morris said…

Good day,
I am RonaId Morris, I saw your profile and I decided to contact you immediately. Can you get back to me on my email (ronmorri01@gmail.com) for full details.  
Regards.

At 6:43pm on March 4, 2012, Louis Ford said…

prepare a pot with a burnished/terra sig surface

Bisque fire to cone 010

pour ferric chloride (x2)   allow to dry

place a crumpled sheet of aluminum foil on a table

put pot on foil

add sea salt, cupper sulphate, drift wood, copper chore boy, miracle grow, etc).....a little goes a long way......choose 1,2,or all....


Wrap the foil tightly around the pot like a baked potato. Try to keep some of the chemicals/organics 'up' on the pot (not just let them fall around the base)

 

FIre in a raku kiln to about 900-1100 degrees F ( I place a shard of bisque with a raku clear glaze on it in the kiln with the potatos.....when it starts to melt/bubble...I turn off the kiln.....SAFETY.....wear a respirator and limit access to the kiln during firing....toxic fumes....wear mask when peeling off the foil as well....experiment...experiment...experiment.

 

 

At 2:44pm on March 2, 2012, Louis Ford said…

That is a nice looking bowl dave.......mind sharing how you built it?  I'm guessing textured slabs placed inside a form?  It would look great as well done in porcelian and left white without glaze.

At 10:07pm on March 1, 2012, Jan Wallace said…

Welcome to the website Dave. I really like the bowl in your profile pic. Look forward to seeing more.

 
 
 

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014