Key West, FL
United States
Simone
Special Red can be found at Ceramic Supply. I put a link on the Glaze Test forum. It will also work better if you do an hour hold at about 1650 F.
Nov 29, 2011
You can email me at ranmcc@msn.com if you have any further questions.
Cancel
Randy McCall
Simone
Special Red can be found at Ceramic Supply. I put a link on the Glaze Test forum. It will also work better if you do an hour hold at about 1650 F.
Nov 29, 2011
Randy McCall
You can email me at ranmcc@msn.com if you have any further questions.