by Susan Stannard
Oct 19, 2023
MC6G Waterfall Brown over Alisa Clausen's Turquoise. In the interior I poured Bill van Gilder's Cream Rust (made with tin oxide but without the RIO). Leaving out the RIO makes a beautiful glassy white glaze.
Hi Susan, I'm just wondering if that turquoise is this one? Alisa Clauson turquoise SS 3894 on glazy.
Your cup is beautiful, love it.
Feb 6, 2024
Hi Alison, yes it is Alisa Clauson's recipe.
Cancel
Alison Moore
Hi Susan, I'm just wondering if that turquoise is this one? Alisa Clauson turquoise SS 3894 on glazy.
Your cup is beautiful, love it.
Feb 6, 2024
Susan Stannard
Hi Alison, yes it is Alisa Clauson's recipe.
Feb 6, 2024