Potters & Sculptors - Making Rock from Mud
Achieving atmospheric glaze effects in electric kilns at mid-fire temperatures, through the layering of sprayed glazes. The starting point recipes are given in two discussions "Strontium Crystal Magic . . ." and "The Companion Glazes"
Website: http://stevenhillpottery.com
Members: 156
Latest Activity: Jul 12, 2018
Started by George Lewter. Last reply by Norm Stuart Sep 29, 2017. 46 Replies 4 Likes
These are the glazes that Steven introduced us to for creating the layered effects for which he is renown. This is the place to post modifications for these glazes, and other glazes that you have found to work well with SCM and SCM for orange. …Continue
Started by Tom Waggle. Last reply by Tom Anderson Oct 17, 2016. 22 Replies 0 Likes
I sent an email out to all group members. I should have just started this thread.I am using Laguna 607 cone 6 stoneware.I am getting pinholes and craters on about 1/3 to 1/2 of my pieces.I contacted Stephen Hill via email to ask him about this. He suggested that I just switch to porcelain as it is the gasses from the impure elements in stoneware body.I have adjusted my bisque schedule to slow down to 100'/hr between 1100' and 1700' ( the temp range where those organic gasses burn off). I am…Continue
Started by Joseph Fireborn. Last reply by Norm Stuart Jul 24, 2016. 5 Replies 0 Likes
This has been created to carry over the conversation that we were having on the discussion comments instead of in a topic. I have copied and pasted the discussion that I created in order of start to current. Please lets move all topics here as it would better be searchable in the future. Comment by Joseph Fireborn I have a question about SH's pots. I have tried using SCM, I get some really nice results, but the glaze surface…Continue
Started by George Lewter Jul 12, 2016. 0 Replies 0 Likes
Numerous members have used SCM and Jen's Juicy Fruit with excellent results. I believe the crystals being objected to are some kind of crystal that is growing in the melt upon cooling, not unmelted strontium poking out of the matrix. The crystals have sharp diamond reflective points which would not be present if they had been even slightly attacked by the glaze fluxes, of which there are plenty, evidenced by the fact that the glaze is very prone to running.My understanding is that …Continue
Comment
Highwater has an earthenware called Bella's Blend that claims cone 6. I just started cone 6 firing using stoneware and had to make an earthenware peice for my aunt and decided to try the leftover Bella's at cone 6. The glazes I'm using worked as well on it as on my stoneware and it vitrified very well. If you fire it any higher than cone 6 you can have some trouble, obviously.
I use Highwaters desert buff and it is made for cone 5/6. I have had no problems with it at all. By the way, I also use vinegar and no slip to attach my handles. I have never, knock on wood, had one crack off:>)
Thanks for all the comments on clay...now I have food for research. Clays to investigate. I have been using Highwaters desert buff and it is acceptable, but I want something with better vitrification at cone 5/6.
Drying slow is always good. Cotton sheets or fabric of any type sometimes works better than plastic.
I use Laguna's Frost and Clay Planet's Icelia porcelain. Both fire to translucent. I've suffered with cracking with both clays until I got a grip on the damp-box and controlling the drying.
I use slip to attach handles and the like. I "wiggle" them in place. What I've found is that it's necessary for me (I work with porcelain) that my pieces dry slowly. My wife and I went to a restaurant supply store and we found an old two door stainless steel cooler/refrigerator for dirt cheap. Plastic interior, shelves and (most importantly) doors with gaskets in good shape. I really need to slow down/control drying especially when doing slip decoration. This applies to handles and such also. When one recycles clay as I do, vinegar can be an issue, it helps to create and ungodly stench in the slip barrel.
I can never remember to buy soda ash, so also use just water with vinegar and have never had problems with cracking as I did when using slip. No scoring, just water/vinegar on each piece to be joined and, as George said, "wiggle and lightly mush the parts together". I like things done as simply as possible, as long as they work.
I'm not using porcelain (b-mix 5). I stopped slipping and scoring about 6 months ago. I use 2 parts water to 1 part white vinegar painted on the surfaces to be joined and I just wiggle and lightly mush the parts together. I have a concern about the sodium silicate in magic water causing a glaze to not absorb at the same rate (thickness) as on pure clay.
Just attended a two day seminar with Steven Hill and he does not use anything but magic water to attach his handles. He made the comment when he used slip he could get cracks also
Steven uses Standard 257 porcelain. I use it now also, but have trouble attaching handles. Everything seems to crack. Been doing handles on cups for 15 years. Don't get it?? I'm going to try some "Magic Water" by Tony Clennell next.. We'll see........
Try Standard clays. Check their website for descriptions. I believe he uses 551, a very plastic porcelain. 563 might be what you're looking for.
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014
© 2025 Created by Andrea Wolf.
Powered by
You need to be a member of Steven Hill Oxidation Project to add comments!