Potters & Sculptors - Making Rock from Mud
Achieving atmospheric glaze effects in electric kilns at mid-fire temperatures, through the layering of sprayed glazes. The starting point recipes are given in two discussions "Strontium Crystal Magic . . ." and "The Companion Glazes"
Website: http://stevenhillpottery.com
Members: 156
Latest Activity: Jul 12, 2018
Started by George Lewter. Last reply by Norm Stuart Sep 29, 2017. 46 Replies 4 Likes
These are the glazes that Steven introduced us to for creating the layered effects for which he is renown. This is the place to post modifications for these glazes, and other glazes that you have found to work well with SCM and SCM for orange. …Continue
Started by Tom Waggle. Last reply by Tom Anderson Oct 17, 2016. 22 Replies 0 Likes
I sent an email out to all group members. I should have just started this thread.I am using Laguna 607 cone 6 stoneware.I am getting pinholes and craters on about 1/3 to 1/2 of my pieces.I contacted Stephen Hill via email to ask him about this. He suggested that I just switch to porcelain as it is the gasses from the impure elements in stoneware body.I have adjusted my bisque schedule to slow down to 100'/hr between 1100' and 1700' ( the temp range where those organic gasses burn off). I am…Continue
Started by Joseph Fireborn. Last reply by Norm Stuart Jul 24, 2016. 5 Replies 0 Likes
This has been created to carry over the conversation that we were having on the discussion comments instead of in a topic. I have copied and pasted the discussion that I created in order of start to current. Please lets move all topics here as it would better be searchable in the future. Comment by Joseph Fireborn I have a question about SH's pots. I have tried using SCM, I get some really nice results, but the glaze surface…Continue
Started by George Lewter Jul 12, 2016. 0 Replies 0 Likes
Numerous members have used SCM and Jen's Juicy Fruit with excellent results. I believe the crystals being objected to are some kind of crystal that is growing in the melt upon cooling, not unmelted strontium poking out of the matrix. The crystals have sharp diamond reflective points which would not be present if they had been even slightly attacked by the glaze fluxes, of which there are plenty, evidenced by the fact that the glaze is very prone to running.My understanding is that …Continue
Comment
Joan - The Critter needs 3 cfm (cubic feet per minute) at 90 psi, according the page on Amazon.com
Critter Siphon Gun on Amazon.com
Just below is the section "Customers Who Bought This Item Also Bought" which shows some $100 compressors with higher PSIs, so the pump or the critter needs a pressure valve to reduce the pressure to the Critter. And these pumps have lower cfms, (a lower flow rate) which is why a compressor has a storage tank.
Based on my limited experience with compressors, another important attribute to consider is the noise level they produce. Sadly, less noise tends to be associated with a higher price.
Comment by Joan Scott 4 hours ago
The Critter Siphon Gun..... wondering which compressor would operate well with this gun? Anyone using this system?
The Critter Siphon Gun..... wondering which compressor would operate well with this gun? Anyone using this ystem?
We have reports of glazemixer.com being temporarily down starting in January. I checked on them a couple of times with the same result. This type of notice without updates usually means permanently down.
The GlazeMixer website is temporarily down for maintenance.
It may take us a few days to finish everything.
If you have any questions, please contact us at customerservice@glazemixer.com
Thank you for your patience.
https://www.glazemixer.com/temporarilydown.htm?aspxerrorpath=/defau...
I am assumeing that Glazemixer is out of business. Does anyone know?
I just joined the group and I'm reading the posts so excuse me if this is answered elsewhere. I the new updated Steven Hill DVD available here in this site? I am not seeing it on the home page of his site. The DVD on the ceramic arts daily site looks like it is not an updated version. Does someone have the link to the updated version? Thanks
Diane, I look forward to seeing your results. I switched to Laguna's Red Rock this year. I love the look of it raw when slightly over fired. I am having to look for new glazes too. I love the look of Steven Hills glazes but spraying isn't an option for at this time. I'm wondering if the same effects could be duplicated by pouring with thin glazes.
anyone know what S Hill's most recent firing schedule is ? I know he changes this, holding at approx 1600 degrees. Trying to program this schedule in my kiln.
Thank you , cp by the pond , now with two bee hives !
The Hanna's Fake Ash I've seen around for years and which I use frequently for Cone 6 oxidation glazing is:
Hanna's Fake Ash:
30 - Whiting
10 - Strontium Carbonate
60 - Redart Clay
Add: 3.5% Red Iron Oxide
3% Yellow Iron Oxide
For Yellow: add 4% Ochre
For Blue Add 1.5% Cobalt Carbonate or around .75% Cobalt Oxide
No Silica in the Hanna's Fake Ash recipe that's been around a long time.
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014