Potters & Sculptors - Making Rock from Mud
Sort by:
| Discussions | Replies | Latest Activity |
|---|---|---|
Does anyone have success dipping the SH Glazes rather than spraying??It appears most of the folks on this forum are spraying Steven's glazes as he recommends. Has anyone dipped the glazes instead? If so, how… Started by Belinda Willis |
12 |
Feb 21, 2012 Reply by Sylvia Shirley |
Strontium Crystal Magic - The Glaze, Variations, Combinations, and AlternativesSteven Hill wrote about the origins of the glaze on the Clayart listserve in 2006. The recipe and variations of it have appeared in many pl… Started by George Lewter |
2 |
Aug 14, 2011 Reply by George Lewter |
What firing schedules have you used with the SH glazes?I finally have the glazes mixed from the March workshop I took with SH. I would like to fire SH glazes in the same kiln with MC6G that I h… Started by martha peddicord |
16 |
Jul 5, 2011 Reply by June Perry |
Steven's Glazes - Tested at Cone 6Is anyone testing some or all of Steven's cone 10 glazes at Cone 6. If so, can you let us know about the results with close up pictures and… Started by George Lewter |
57 |
May 1, 2011 Reply by martha peddicord |
Other Glazes that Develop Complex SurfacesI've been testing Richard Busch's Nutmeg (from Ceramics Monthly and online at Ceramic Arts Daily) both single fired and on bisque. I tried… Started by George Lewter |
4 |
Nov 4, 2010 Reply by George Lewter |
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014
© 2025 Created by Andrea Wolf.