How to prevent database pollution or how to clean up the insight-Live data. Your views please.

My main reason to use Insight-Live is the chemistry calculation and comparison between recipes. Many recipes entered into the database fail to calculate chemistry, because the materials are misspelled, named differently or the colouring oxides are included. I cannot change the recipe when I am not the owner. So what should I do? Let's take Leach Clear as an example.

 

Material "frit,Ferro 3124" does not exist in the Materials data  and hence the calculation fails.

I could

1- copy the recipe and change it but that results in recipe pollution

2- ask the owner to change it, but I hate to bother him, especially since he entered very many recipes

3- add "frit, Ferro 3124" to  Our Materials with a reference to Ferro Frit 3124 and do something similar for "feldspar, Custer" and "kaolin, calcined".  This pollutes the Our Materials data.

On top of this solution 3 does not work when coloring oxides or eg. bentonite are specified as materials and not as additions.

And I still have to revert to solution 1 when I need to replace a material that I cannot buy here by one that I can get.

So, what do you think the best approach would be?

Views: 1033

Replies to This Discussion

I have the "Our Managed Materials"

China Clay - linked to the chemistry for generic Kaolin

Wood Ash - linked to Digitalfire chemistry for Hardwood Ash

there's a huge variance in wood ash, but this is what "Wood Ash" will be unless otherwise specified.

There are others to choose from.

Unless I missed some, all of the glaze 708 recipes in our Insight-Live database contain only linked raw materials. A number of these glazes include one or more color variations.

The only remaining problems are glazes where the Additions are not separated from the recipe, primarily in the imported glazes. I won't be changing those unless I find some pressing need to do so on an individual basis.

I never dreamt my post would lead to this spring cleaning :)  You did a lot of work, thanks very much. The recipes are so much more useful when it is easy to compare the chemistry.

Norm Stuart said:

Unless I missed some, all of the glaze 708 recipes in our Insight-Live database contain only linked raw materials. A number of these glazes include one or more color variations.

The only remaining problems are glazes where the Additions are not separated from the recipe, primarily in the imported glazes. I won't be changing those unless I find some pressing need to do so on an individual basis.

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2025   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service