Comment
The single firing group has been pretty inactive. If I were to guess why, it would be because of the little difficulties that can be overcome one by one, but taken in total they seem to make the process more problematic than simply bisquing and glaze firing like most people do.
I mostly have gone back to conventional firing myself, but if I have a piece that needs a superfast turnaround I will occasionally add the single fire pieces to a normal load and then run a single-fire schedule on the kiln heating very slowly,through 500 degrees and through the 1000-1400 degree range and then just my normal firing schedule.
The biggest problems seem to be when glazing the raw ware. Cracks in the thin areas showing up when drying, crawling before and during firing, and bloating during the firing.
Not all clay bodies will tolerate the process, not all glazes will work well. But if you wanted to develop a line of pieces that you plan to reproduce on a production scale, single-firing could make economic sense. I don't think it makes sense for an art potter constantly making entirely new creations and changing glazes and techniques.
I'm sure Steven Hill is still single-firing, but I read recently that he has upped his firing temperature back up to cone 8. See the article on his website at http://www.stevenhillpottery.com/glazing/firing/
Feel free to ask questions. I will post this reply to the group.
Thanks. One of the poorly performing glazes was Raw Sienna from the MC6 book, a semi-matte glaze. On the other hand I used "dry red brown" a high iron matte glaze, and it did fine. This was an interesting experiment. I'll have to think about whether I want to continue single firing.
I doubt the interrupted firing caused crawling. By cone 1 everything was more than bisqued, yet very few cone 6 glazes should show any sign of fluidity.
The few times we've done once-fired pieces, I've found the more fluid glazes work better probably because they heal if they get blown-off in places when the greenware off-gasses.
I fired my first raw glazed, once fired load. Everything went wrong. I had a power failure at cone 1. The kiln temperature was 198F when the lights came back on. I re-fired to cone 6. There was serious crawling of one glaze and mild to moderate in others. A shino glaze worked like a charm. Does anyone know whether the re-firing may have caused the crawling. I assume it was a poor glaze / clay fit.
I put his on the main wall - http://cone6pots.ning.com/photo/dsc-2571-7?xg_source=activity
I am working in a community studio, and they are exploring single fire right now. No real issues at this point and the clay is the cone 6 b-mix from laguna.
Will let you know once I can single fire my own work, as I am using cassius by aardvark and just moved to electric brown by laguna (was hearthstone from mile hi in denver but they do not consistently have the clay).
~What clays are folks using at the cone 5-7 range??? I am looking for info about vitrification at that temp.
I first learned about single fire with Dennis Parks at a wrkshp in NH in '75... waste oil kiln too. He applied glaze to dried pots. quickly inside then sponge the outside bottom with clear water to equalize pressure then quickly dip the outside. timing was essential. I have not done it in many yrs, my forms are too complicated to withstand the stress. Have a great day.
Hello everyone. My name is Ian. I am the owner of Cloud House Pottery in Delray Beach, Fl. I mailny do Raku. But when I fire to cone 6, I usually single fire. I would like to get to know all of you & share experiences
I am still pursuing single firing as my kiln is very small and I have been trying a couple of different methods as spraying was still leaving too much moisture. My biggest problem is with the pieces cracking in the green state from the moisture in the glaze. Recently I've tried brushing the glaze on in small sections and drying quickly with a heat gun. The glaze doesn't go on smoothly and I've tried adding 2% CMC gum to my glazes which helps brush-ability and toughens the glaze, enabling me to get it to the kiln but it still clumps on the pot. I am having success with glazing my pots while still leather hard which is working much better. I's tricky to get enough glaze on the pot and I am having trouble with splitting in my large mugs along the seam which I am looking at as a design issue. Bowls and open forms seem to do really well with this and I wondered if anyone else is dealing with this issue and finding solutions?
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014