"This is my current firing schedule for newly glazed and still damp ware. I'm current…"

George Lewter replied Oct 31, 2011 to Firing cycle for single firing

19 Sep 7, 2015
Reply by Melissa Mead

"I'm doing a single fire today with my new Orton controller - No constant messing wit…"

George Lewter replied Apr 30, 2011 to Firing cycle for single firing

19 Sep 7, 2015
Reply by Melissa Mead

"Over in the Main discussion area is a similar topic "Raw Glaze Problem Solving"."

George Lewter replied Apr 13, 2011 to Glaze Application for Single Firing

5 Jan 2, 2012
Reply by Anne Cunningham

"The following were moved from General Comments on the Single Firing Group main page …"

George Lewter replied Dec 15, 2010 to Firing cycle for single firing

19 Sep 7, 2015
Reply by Melissa Mead

"Thanks, Victoria for linking to that article. I was not sure what bloating is until…"

George Lewter replied Nov 21, 2010 to Firing cycle for single firing

19 Sep 7, 2015
Reply by Melissa Mead

""

George Lewter replied Nov 8, 2010 to Let's Get Started with Single Firing

15 Nov 8, 2010
Reply by George Lewter

"Comparison Tests from My Last Kilnload I wanted to try single firing some pieces usi…"

George Lewter replied Oct 17, 2010 to Let's Get Started with Single Firing

15 Nov 8, 2010
Reply by George Lewter

"Suggested schedule for a cone 8 firing. 1 200 deg/hr to 220 hold 1 to 3 hrs dependi…"

George Lewter replied Sep 15, 2010 to Firing cycle for single firing

19 Sep 7, 2015
Reply by Melissa Mead

"I fired another load that contained some raw glazed pots, and though the glaze effec…"

George Lewter replied Oct 28, 2009 to Let's Get Started with Single Firing

15 Nov 8, 2010
Reply by George Lewter

"My results were not perfect, but they were very encouraging. The pots I glazed leath…"

George Lewter replied Oct 5, 2009 to Let's Get Started with Single Firing

15 Nov 8, 2010
Reply by George Lewter

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2024   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service