I'm still in the learning stage re using rutile.

First question: Can two bowls that have a cobalt oxide-colored slip plus an added rutile wash be stacked rim to rim in a bisque fire? 

The effect I wanted from the rutile was drips / runs of the cobalt slip. The bowls are Little Loafers clay (white); when they were soft leather-hard I put them on the wheel and brushed on the slip, starting from the rim and spiraling to the bottom. Then with another brush I applied the rutile wash over it. I'm going to bisque fire them today about 1 p.m., hence the time-sensitive part. 

Second question: What's a good formula for adding rutile to a batch of colored slip? And should I add powdered rutile, or rutile wash?

Thanks very much for help.

Views: 1103

Reply to This

Replies to This Discussion

Both rutile and cobalt oxide/carbonate are very refractory and will not melt in a bisque - but other ingredients you add to the slip might.

Granular rutile fired to cone 6 doesn't change much in most glazes, remaining as the same brown spots they looked like when you add them to the glaze.

Granular rutile or ilmenite added to clay results in the speckled brown spots similar to those seen in fired Laguna Speckled Buff clay.  Unfired that clay is an odd pink color.

WC-403 Speckled Buff Clay

The only way to know what things will look like in advance is to fire test tiles.  Test tiles are a very underused tool.  When you refer to a rutile "wash", what does this mean to you other than rutile and water?

Hi, Norm - thanks for your reply. To me a rutile wash is rutile + water. But actually I bought a small bottle of Mayco rutile wash to experiement with, and I don't know what else is in there. I take it from your question that if I'm making my own using powdered rutile, there would be other materials included.

The slip I used is just the clay body + water.

I could have safely gone ahead with firing the bowls rim to rim, I know now, and sort of thought that at the time. But I'm (over)cautious when I do something in ceramics I haven't done before -- need to get over that, I think! Anyway, I took out the top bowl, and started my bisque a few hours ago. Oh, and of course yes, to test tiles. ;)

Thanks again.

I've been using a 20 year old bag of Dark Rutile for glazes which always created nice strands, as in the Honey glaze below.

Once we began using a newly purchased bag of calcined Light Rutile, we've created glazes which are uniformly opacified rather than strands.  I've been able to recreate so of the strand behaviour by reducing the amount of rutile by about 2/3 - but the artistic result is negligible when compared to our old bag of rutile.  Most annoying.

We'll purchase a bag of Dark Rutile, but I don't have high expectations for recreating the original look.  It appears that all Rutile in North America is sold by the TAM subsidiary of the Ferro Corp, consisting of a blend of Australian and American Rutile.

Rutile is being produced by Sierra Leone, likely the source of our very old bag, but I can't find a place which sells it.  Does anyone  have any ideas?

Honey Glaze, made with very old Rutile and a new bag of Light Rutile

The rutile supply I have gives the strands you like. I believe it came from US Pigment.

Thanks so much Nadine, I'll give Sayed Abbas a call.  He does sell best quality material.

Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Your final price could be less or more - things change.

American Weigh Black Blade Digital Scale, 1000g X 0.1g $11.08 

For the non-digitally inclined the old standard Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2021   Created by George Lewter.   Powered by

Badges  |  Report an Issue  |  Terms of Service