Does anyone use the little test sized sieves when mixing small test batches? I have found that sometimes that I get spotting or irregular runs when I use only a hand blender for small test batches. The same recipes don't get this when I mix a full batch and use the proper sieves. Do you find the small sieves useful? Or do you use a homemade version? Other?

Views: 210

▶ Reply to This

Replies to This Discussion

i find those little sieves very useful.  i can place them over a yogurt cup and use a soft rubbber spatula to press the material thru. i usually do it twice to make sure i have all material pushed thru. i use either the 60 or 80 mesh to get decent results

We have a 100 mesh and a more annoying 120 mesh which we use for large batches and small batches of glaze over a bowl or a bucket.

1.) Wollastonite is always problematic because it's fibrous so takes quite a while to get through any mesh, and doesn't respond to a blender.

2.) Even clays can leave lumps after mixing with a stick blender.  I just made some wet clay into colored slip with a stick blender two days ago and I can still see the occasional tiny lump, smaller than a peppercorn, as I stir the slip.

3.) Bentonites need to be well mixed with the other dry ingredients prior to adding the dry mix to water, otherwise you'll be spending a lot of time with the sieve. Bentonites wet faster with hot water.

If you want to use chemistry to solve the problem without a sieve, use a wetting agent like liquid Tide detergent to your glaze mix.

Thanks for your replies. I didn't see them where I usually order my clay from but see them at a few of the other online shops. I ran a small 200 gr test through a large sieve last week but it seemed that almost as much glaze was left in the sieve and big bowl as was left for testing, so will put a little one on my shopping list. 

I hadn't heard of using a wetting agent ... thanks for the tip .... I just did a quick google to learn more about wetting agents. 

A wetting agent aka detergent aka surfactant merely reduces the surface tension of water so it can spread easier through a solid.

A washing machine detergent like Tide is designed to minimize any foam. If you mistakenly used a dish washing soap with foaming agents, you'd end up with bubbles every time you stirred the glaze.

There is always some glaze caught in the mesh, but I just use the flexible rib or a spatula to empty the bowl.  Glaze making has a lot of overlap with cooking.

"Glaze making has a lot of overlap with cooking", I agree! Having been a Home Ec teacher I also find that working with clay has quite the overlap with sewing! 

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service