I found a small 115V kiln on my Craigslist and I think it would make a great test kiln.  I'm limited in space right now but I would like to create my own glazes and I've been thinking of buying it to at least be able to run test tiles through.  What do y'all think?  I'm sure some of you have experience in this type of thing.  Any advice would be greatly apreciated.

-John

Views: 240

▶ Reply to This

Replies to This Discussion

Hi John,
I think a small test kiln is always a good idea. It's best if it mimics your actual regular kiln as close as possible so that if you get something really amazing in the test kiln you can duplicate it on a larger scale. I have to stick test tiles in with regular loads and it is frustrating to have to wait sometimes. I actually had a small kiln made for me by Vulcan kilns as I had an extra controller to put on it. Had to wait though to get the s-type tc to go with it. Hopefully I can get it put together over memorial day. I had it made just big enough to also do Christmas ornaments in as well. There's just never enough hours in the day!

I have a 110 20 amp skutt that I have for sale,  the reason is that it takes FOREVER to get to cone 6,  no venting system.  I cannot plug it to my Skutt controller so it is not a replica of my big kiln and therefore I don't trust the tests...I suggest that you sacrifice some space in your standard kiln for test glazes.

Nadine

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014