Ruined cups - Electric Mid&Hi Fired Ceramics2024-03-29T11:13:50Zhttps://cone6pots.ning.com/forum/topics/ruined-cups?feed=yes&xn_auth=noPhotos of the fired ware?
Ph…tag:cone6pots.ning.com,2021-04-18:2103784:Comment:1704702021-04-18T03:54:12.959ZNorm Stuarthttps://cone6pots.ning.com/profile/NormStuart
<p>Photos of the fired ware?</p>
<p></p>
<p>Photos of the kiln interior wouldn't hurt either.</p>
<p>Photos of the fired ware?</p>
<p></p>
<p>Photos of the kiln interior wouldn't hurt either.</p> This was during a cone 05 bis…tag:cone6pots.ning.com,2021-04-01:2103784:Comment:1706582021-04-01T23:52:53.592ZRobert spicerhttps://cone6pots.ning.com/profile/Robertspicer
This was during a cone 05 bisque firing