red pink purple mauve glaze - Electric Mid&Hi Fired Ceramics2024-03-29T14:36:31Zhttps://cone6pots.ning.com/forum/topics/red-pink-purple-mauve-glaze?commentId=2103784%3AComment%3A102170&x=1&feed=yes&xn_auth=noI've had good and bad firingsā¦tag:cone6pots.ning.com,2014-03-30:2103784:Comment:1021702014-03-30T21:01:10.000ZWyndham Dennisonhttps://cone6pots.ning.com/profile/WyndhamDennison
<p>I've had good and bad firings with chrome pinks. The reason for bad firings is they don't like any zinc in the atmosphere or adjoining pots....zinc kills pink(chrome/tin).</p>
<p>Good results came from a heavier application, test to see what works best. It may take several firings to dial it in.</p>
<p>Google "chrome red glaze recipes" and you will find several try testing several.</p>
<p>Wyndham</p>
<p>I've had good and bad firings with chrome pinks. The reason for bad firings is they don't like any zinc in the atmosphere or adjoining pots....zinc kills pink(chrome/tin).</p>
<p>Good results came from a heavier application, test to see what works best. It may take several firings to dial it in.</p>
<p>Google "chrome red glaze recipes" and you will find several try testing several.</p>
<p>Wyndham</p>