I have been away for awhile.  We had to get our house ready to sell so that we could build a new one.  Anyway, I am going to have my kiln room in the 3rd car garage and I will have my gas kiln just outside the door.  Right now the kiln is clear in the back of the storage unit, but the contractor wants to know the Btu's so that he can appropriately size the gas line for it. If I could get to the kiln it would be easy to get the specs off the name plate, but I can't get to it.  It is approx 28" wide & 36" tall.  I don't even remember the model number.  It has a 4 burner system that is part of the base and it is a downdraft system.  Any help would be greatly appreciated.  I called Skutt and they don't have any info and I haven't had any luck googling it, especially without a model number.  Like I said, any help would be most welcome so I know what to tell the contractor.  J

Views: 200

Reply to This

Replies to This Discussion

I would guess the range of 250,000 - 300,000 btus to be in actual ballpark and 400,000 would make a reasonable safety allowance. The Olympic 28 d X 27 h - maxes out at 280,000 btu, but it is an updraft.

If the size you noted is the inside or stacking space, then 500,000 might be closer to what you need. 

Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service