<p>I'm trying to use only a little of pheatine. The shop that gave me it said that can have a little of flux effect.</p>
<p>In my first experiment I did not use pheatine and the glazes were quite good.</p>
<p>I fire at 1240°C: I think it can be between cone 6 and cone 7. Very near to cone 7 probably.</p>
<p>Thanks</p>
<p>I'm trying to use only a little of pheatine. The shop that gave me it said that can have a little of flux effect.</p>
<p>In my first experiment I did not use pheatine and the glazes were quite good.</p>
<p>I fire at 1240°C: I think it can be between cone 6 and cone 7. Very near to cone 7 probably.</p> Pheatine paste may itself be…tag:cone6pots.ning.com,2021-02-25:2103784:Comment:1700352021-02-25T23:13:35.946ZNorm Stuarthttps://cone6pots.ning.com/profile/NormStuart
<p>Pheatine paste may itself be bentonite and water.</p>
<p>Fire some pheatine paste by itself. If it leaves no trace, it is an organic suspender rather than mineral like bentonite.</p>
<p>Smcetites like bentonite contain fluorine which is an important flux, without which ash glazes may not do much at cooler cones.</p>
<p></p>
<p>Pheatine paste may itself be bentonite and water.</p>
<p>Fire some pheatine paste by itself. If it leaves no trace, it is an organic suspender rather than mineral like bentonite.</p>
<p>Smcetites like bentonite contain fluorine which is an important flux, without which ash glazes may not do much at cooler cones.</p>