Materials substitution - Electric Mid&Hi Fired Ceramics2024-03-28T14:56:40Zhttps://cone6pots.ning.com/forum/topics/materials-substitution?feed=yes&xn_auth=noYes, gillespie borate will fi…tag:cone6pots.ning.com,2020-12-19:2103784:Comment:1677382020-12-19T01:33:31.438ZNorm Stuarthttps://cone6pots.ning.com/profile/NormStuart
<p>Yes, gillespie borate will fire very similar to gerstley borate.</p>
<p></p>
<p>Each batch of gerstley borate used to be slightly different as they dug through a different area of the deposit.</p>
<p>Yes, gillespie borate will fire very similar to gerstley borate.</p>
<p></p>
<p>Each batch of gerstley borate used to be slightly different as they dug through a different area of the deposit.</p>