After reading "Mastering Cone 6 Glazes" I wanted an easy reference to the example glazes.

Click here to purchase an  eBook  version of this reference by Ron Roy and John Hesselberth.  Glaze Photos

My Excel spreadsheet  MC6G.xls  includes these glazes along with:

a.)  a listing of ceramic material we stock at our studio;

b.)  the cost per pound of each material, linked to the glaze recipes for cost accounting;

c.)  an Orton Cone Chart with references to the various temperatures where various reactions occur.

If you want to use this as a template for your own use, unprotect each worksheet.  There is no password required to unprotect the spreadsheet.  Depending on your version of Excel, Unprotect Worksheet is listed under either the Tools or the Review menu.

CoverPotSection

Views: 2079

Attachments:

▶ Reply to This

Replies to This Discussion

Norm, 

i actually came here this am to start a discussion on MC6 specifically.  Thanx for starting this one . Question - is that your own pic ? 

cp - by the pond, where the geese finally landed, and i think we have an Ibyss (sp)  also.

The expert photo of the best you can achieve with Waterfall glaze is from the book cover.

Waterfall glaze more typically looks like this.  You need to apply it quite thickly to look like the book cover.  You need to apply less when you're using an iron-rich dark clay.

We now slow-cool our kiln far slower at 1/3 the speed recommended by Roy and Hesselberth, so Waterfall now looks like this.  Someday we'll have to make some more with 15% Ferro 5301 to see what it comes out like when it has enough flux and glass to be an ultra-slow-cool glaze. 

As you can see when cooled at 50 F per hour within the 1,800 F to 1,500 F range the glass level falls below the top layers of crystallization, which is typically not that attractive  - unless you like that sort of matte.



Norm Stuart said:

The expert photo of the best you can achieve with Waterfall glaze is from the book cover.

Waterfall glaze more typically looks like this.  You need to apply it quite thickly to look like the book cover.  You need to apply less when you're using an iron-rich dark clay.

We now slow-cool our kiln far slower at 1/3 the speed recommended by Roy and Hesselberth, so Waterfall now looks like this.  Someday we'll have to make some more with 15% Ferro 5301 to see what it comes out like when it has enough flux and glass to be an ultra-slow-cool glaze. 

As you can see when cooled at 50 F per hour within the 1,800 F to 1,500 F range the glass level falls below the top layers of crystallization, which is typically not that attractive  - unless you like that sort of matte.

norm, thanx again

i am going to use the base glazes and see how they work

thanx

cp

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service