Gravity feed spray guns? - Electric Mid&Hi Fired Ceramics2024-03-28T17:34:01Zhttps://cone6pots.ning.com/forum/topics/gravity-feed-spray-guns?feed=yes&xn_auth=noI like to use the DeKups disp…tag:cone6pots.ning.com,2014-12-10:2103784:Comment:1170362014-12-10T15:56:17.673ZCyndy Littletonhttps://cone6pots.ning.com/profile/Cyndyshorter
<p>I like to use the DeKups disposable cups system for my spraying. This allows you to interchange the glazes without having to use multiple spray guns. In addition, you can store glazes for a short time in them if doing multiple days of glazing. I purchased them from TCPGlobal.com.</p>
<p>I like to use the DeKups disposable cups system for my spraying. This allows you to interchange the glazes without having to use multiple spray guns. In addition, you can store glazes for a short time in them if doing multiple days of glazing. I purchased them from TCPGlobal.com.</p> I'm not a fan of HF, but the…tag:cone6pots.ning.com,2014-12-09:2103784:Comment:1168992014-12-09T06:18:35.146ZScott Marshallhttps://cone6pots.ning.com/profile/ScottMarshall
<p>I'm not a fan of HF, but the reviews on these disposable paint cups are pretty good. They come with adapters to fit most HVLP paint guns, and you can always use a bit of teflon tape on the threads for leaks. For less than the price of lunch you get 5 disposable plastic paint cups - I might give this a try.…</p>
<p>I'm not a fan of HF, but the reviews on these disposable paint cups are pretty good. They come with adapters to fit most HVLP paint guns, and you can always use a bit of teflon tape on the threads for leaks. For less than the price of lunch you get 5 disposable plastic paint cups - I might give this a try. <a href="http://www.harborfreight.com/5-piece-air-spray-gun-disposable-paint-cups-97098.html" target="_blank">http://www.harborfreight.com/5-piece-air-spray-gun-disposable-paint-cups-97098.html</a></p>
<p>I think SH shows the Titan Paint Cups in his surface video - about $10-15 each.</p> TCP Global guns are now avail…tag:cone6pots.ning.com,2014-09-08:2103784:Comment:1115442014-09-08T02:23:43.406ZGeorge Lewterhttps://cone6pots.ning.com/profile/GeorgeLewter
<p>TCP Global guns are now available at Amazon.com. If you order via these links, the cone6pots network will earn a small commission on your order.</p>
<p><a href="http://storage.ning.com/topology/rest/1.0/file/get/3127169705?profile=original" target="_self"><img class="align-left" src="http://storage.ning.com/topology/rest/1.0/file/get/3127169705?profile=original" width="160"></img></a></p>
<p><a href="http://www.amazon.com/TCP-Global%C2%AE-Brand-Professional-Regulator/dp/B001OZMOV8" target="_blank">TCP Global® Brand Professional HVLP Spray Gun with 1.4mm Fluid Tip and Regulator</a></p>
<p>This is a good tip…</p>
<p>TCP Global guns are now available at Amazon.com. If you order via these links, the cone6pots network will earn a small commission on your order.</p>
<p><a href="http://storage.ning.com/topology/rest/1.0/file/get/3127169705?profile=original" target="_self"><img src="http://storage.ning.com/topology/rest/1.0/file/get/3127169705?profile=original" width="160" class="align-left"/></a></p>
<p><a href="http://www.amazon.com/TCP-Global%C2%AE-Brand-Professional-Regulator/dp/B001OZMOV8" target="_blank">TCP Global® Brand Professional HVLP Spray Gun with 1.4mm Fluid Tip and Regulator</a></p>
<p>This is a good tip size for glazes sieved at 60 mesh or finer. At the time of this posting it ships free to Amazon Prime members. Price at the time of this posting - $39.96</p>
<p></p>
<p></p>
<p></p>
<p></p>
<p></p>
<p></p>
<p></p>
<p><a href="http://storage.ning.com/topology/rest/1.0/file/get/3127169620?profile=original" target="_self"><img src="http://storage.ning.com/topology/rest/1.0/file/get/3127169620?profile=original" width="160" class="align-left"/></a><a href="http://www.amazon.com/TCP-Global%C2%AE-Brand-HVLP-Spray/dp/B001N1E9Y8" target="_blank">TCP Global® Brand HVLP Spray Gun Set</a> - 3 Sprayguns with Cups, Air Regulator, Stand, & Maintenance Kit for all Auto Paint, Primer, Topcoat & Touch-Up, One Year Warranty</p>
<p>This might be a good setup for someone serious about spraying layered glazes. Two sizes of tips (1.4 & 1.8 mm) for base coat and general glaze application, and a detail gun for smaller areas. Note that the detail gun is <strong>not an airbrush,</strong> and will not be making 1/8 inch lines. This set ships free with Amazon Prime membership. Price at the time of this posting - $69.96</p> The ones pictured in his vide…tag:cone6pots.ning.com,2012-02-29:2103784:Comment:574062012-02-29T21:34:40.595ZLinda Staufferhttps://cone6pots.ning.com/profile/LindaStauffer
<p>The ones pictured in his video were ones with a plug for the hole in each end of the cup and a stand to store the cup. </p>
<p>The ones pictured in his video were ones with a plug for the hole in each end of the cup and a stand to store the cup. </p> I haven't seen those there, g…tag:cone6pots.ning.com,2012-02-29:2103784:Comment:572072012-02-29T17:23:01.258ZJohn Loweshttps://cone6pots.ning.com/profile/JohnLowes
<p>I haven't seen those there, good heads up for my next visit.</p>
<p>I haven't seen those there, good heads up for my next visit.</p> I know in his workshops he re…tag:cone6pots.ning.com,2012-02-29:2103784:Comment:572052012-02-29T17:19:16.867ZJohn Loweshttps://cone6pots.ning.com/profile/JohnLowes
<p>I know in his workshops he recommends guns from TCP Global such as this set:</p>
<p><a href="http://www.amazon.com/TCP-Global%C2%AE-Brand-HVLP-Spray/dp/B001N1E9Y8" target="_blank">tcp global spray gun set</a></p>
<p>The <a href="http://www.amazon.com/DeVilbiss-DPC601-DeKups-Diposable-Cup/dp/B0015PKQ5I" target="_blank">DevilBiss DeKups Disposable Cup System</a> may be the system in his video (I have not seen the video)</p>
<p>I would call and ask if they also carry the adapters for your…</p>
<p>I know in his workshops he recommends guns from TCP Global such as this set:</p>
<p><a href="http://www.amazon.com/TCP-Global%C2%AE-Brand-HVLP-Spray/dp/B001N1E9Y8" target="_blank">tcp global spray gun set</a></p>
<p>The <a href="http://www.amazon.com/DeVilbiss-DPC601-DeKups-Diposable-Cup/dp/B0015PKQ5I" target="_blank">DevilBiss DeKups Disposable Cup System</a> may be the system in his video (I have not seen the video)</p>
<p>I would call and ask if they also carry the adapters for your spraygun (these are at the bottom of the page.) I should think the disk filter could be tossed as most glazes will clog a filter.</p>
<p>John Lowes</p>
<p><em>Note: This post edited by George Lewter. John's links above to TCP Global were broken. After finding the products on the TCP Global website, I noticed the same products costing less at Amazon, so I redirected the links there. 9/7/2014</em></p> Linda
I've seen some at Harbo…tag:cone6pots.ning.com,2012-02-28:2103784:Comment:571752012-02-28T22:14:38.740ZRichard Hoffmanhttps://cone6pots.ning.com/xn/detail/u_3cjdfxmedm190
<p>Linda</p>
<p>I've seen some at Harbor Freight but have never tried them on my spray gun to see if they fit.</p>
<p>Rich Hoffman</p>
<p>Linda</p>
<p>I've seen some at Harbor Freight but have never tried them on my spray gun to see if they fit.</p>
<p>Rich Hoffman</p>