I am interest in knowing if anybody has done this. I'm thinking of pit firing some 06 bisqued pots, glazing with cone 6 clear and then firing to cone 6.  I am using B mix and Soldate 60 Laguna Clay mixed together. Is this possible and/or practical? Thanks in advance for any advice.

Views: 460

Reply to This

Replies to This Discussion

You would lose all the smoke blackening, and if you used copper or iron to get colors, they would be modified by the glaze. If you are just looking for a bisque, then this would be one way to do it.

Thanks for the reply. I don't want to lose the patterns from the pit firing so this plan of action isn't going to work! Back to the drawing board...

Wondering why you want to refire the pit fired pots to cone 6. Do you want to vitrify them? You could seal them with tile sealant to make them water proof although I doubt they would be food safe.


Scott Shaffer said:

Thanks for the reply. I don't want to lose the patterns from the pit firing so this plan of action isn't going to work! Back to the drawing board...

I am working on making bonsai pots and really like the patterns/colors I get with pit firing. I do want to make them water proof and safe for the bonsai trees. I don't want stuff leaching into the trees and I figured that firing to cone 6 with a clear glaze would accomplish this. 

I really love the pit fired patterns as well. My profile picture is a pot I barrel fired and got an amazing blue color, don't know how! I have used plastic liners and planted into barrel fired pots with success. No leaking when watered and the plant is doing great. Another option may be to burnish the pot before bisque firing &/or coating with t-sig, both which help seal the surface. Good luck and let us know how you make out.

Scott Shaffer said:

I am working on making bonsai pots and really like the patterns/colors I get with pit firing. I do want to make them water proof and safe for the bonsai trees. I don't want stuff leaching into the trees and I figured that firing to cone 6 with a clear glaze would accomplish this. 

Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service