Hi every one,

I have a dilema. I have been producing this lotus pattern with Raku quite successfully.
I would really like to be able to do the same thing with a stoneware firing so that the pieces are functional but still using glazes not underglazes.

I can't quite get my head around it.

I draw the pattern then tape it using auto tape. apply the turquoise and clear crackle, remove the tape and it's ready to fire. The reduction in the bin makes the lines black.

With stoneware I draw, tape, glaze the lotus and then I'm stuck because I don't want the raw clay where the tape was. I've tried liquid wax but that's hopeless. I don't want the 2nd glaze to go over the pattern because I'm sure it would meld and disappear.

Does anyone have any ideas. Regards, Jenny

Views: 199

▶ Reply to This

Replies to This Discussion

You could always use a black stoneware.  They are usually not cheap & they will make the rest of your glazes look different. Usually more dark & metallic.  You could also use black slip.  I use the black slip from Stone Mountain Clay.  I have brushed it & also sprayed it.  jhp

Thanks Jeff,
I'll have to look for black stoneware here in Australia.
I've tried black slip but it doesn't seem to react very well to the glazes, peels off and look like a crispy critter.

jenny

Hi Jenny, you could paint a black glaze on with a brush after removing the tape.  If you don't have a black glaze you could make one by adding black mason stain to your clear glaze.  Good luck.  Post you test and let us see what you come up with.

-chantay

I did try to do the taping put the coloured glaze on and then liquid wax. Very difficult. I used a black glaze called licorice. It flowed over most of the pattern, so much so that I couldn't fiqure out which bowl it was until I referred to my notes. I will try it brushed on though and see.
Thanks for the suggestion.

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by