This is a modification of a glaze from Glazes Cone 6 by M Bailey
 It gives a real nice matt blue break where thick and  matt green where thin.
 My problem is that it always looks fine on the test tiles I fire but some of the  pots I fire show craters (not pin holes) and fish eyes, while others, from the same kiln load,  look fine. A second firing sometimes solves the problem but not always. Any thoughts?
             
             Neph Sy     69
             GB              9
             Ball Clay       8
             Whiting        5
             Silica           5
             Rutile           2
             Cobalt Carb   1
             Titanium O2  1

Views: 158

▶ Reply to This

Replies to This Discussion

 Thanks, Brian.

I probably need to re-formulate in a systematic way. I'll start with the GB and instead of running test tiles , I'll make some mugs or something so I have a better chance of catching it, since it never showed up on the test tiles.

I always do 300 gram test  batches. This is a convenient weight for the double pan balance I use. My fear is that the larger batches I make are less accurate than the test batches, since I use a digital postal scale which is only accurate to about 5 grams . I try to compensate for the built in inaccuracy of the postal scale by weighing the smaller amounts of ingredients on the double pan that has a 1/10 gram accuracy.

It seems like any real glaze you would want to use should be able to tolerate a couple of percent slop in the  accuracy of the formulation... at least for the major components.

I am not a production potter so I make up only about ten pounds of glaze at a time. I also mix the new batch in with anything remaining of the old batch. I don't know if this is a good idea or not, but I hate to waste it. I run a test tile on the final mix to make sure it fires alright.

I brush the glaze on rather than dipping. The glaze breaks blue where thick, and I try to encourage this by brushing on thicker in some areas.

▶ Reply to Discussion

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service