All Discussions Tagged 'specific' - Electric Mid&Hi Fired Ceramics2024-03-28T11:55:26Zhttps://cone6pots.ning.com/forum/topic/listForTag?tag=specific&feed=yes&xn_auth=nospecific gravitytag:cone6pots.ning.com,2016-12-07:2103784:Topic:1387662016-12-07T13:52:14.403ZRobin Cherfanehttps://cone6pots.ning.com/profile/RobinCherfane889
<p>Does anyone know what a good specific gravity is for Cushing's Satin White Matte? I'm mixing up a 5000g batch and don't know how much water to start with. I did a 100g test batch using the "solo cup" line, which came out nice but too little to measure sp. gr. </p>
<p>Does anyone know what a good specific gravity is for Cushing's Satin White Matte? I'm mixing up a 5000g batch and don't know how much water to start with. I did a 100g test batch using the "solo cup" line, which came out nice but too little to measure sp. gr. </p>