All Discussions Tagged 'controlled' - Electric Mid&Hi Fired Ceramics2024-03-28T20:08:16Zhttps://cone6pots.ning.com/forum/topic/listForTag?tag=controlled&feed=yes&xn_auth=noScheduling slow-cool cycles after you have reached temptag:cone6pots.ning.com,2016-03-10:2103784:Topic:1283812016-03-10T20:40:09.084ZIan Hall-Houghhttps://cone6pots.ning.com/profile/IanHallHough
<p>Hi all - I did not schedule a slow cooling cycle when I fired the kiln, but decided after it had reach temp that I wanted to try it. Is there a way you know of to program this way? I was planning 500f/h to 1900, then 150F/h to 1400, but when I press start it thinks the program is finished. Thoughts?</p>
<p>Hi all - I did not schedule a slow cooling cycle when I fired the kiln, but decided after it had reach temp that I wanted to try it. Is there a way you know of to program this way? I was planning 500f/h to 1900, then 150F/h to 1400, but when I press start it thinks the program is finished. Thoughts?</p>