All Discussions Tagged '#positve' - Electric Mid&Hi Fired Ceramics2024-03-29T07:36:47Zhttps://cone6pots.ning.com/forum/topic/listForTag?tag=%23positve&feed=yes&xn_auth=noDarvan/dispersant & slip ..is that the need 4 non-Newtonian thixotropic character reversel in wheelwork.tag:cone6pots.ning.com,2019-08-13:2103784:Topic:1541442019-08-13T10:50:41.389ZAndre Johann Strydomhttps://cone6pots.ning.com/profile/AndreJohannStrydom
<p>We have a lot of recycled white slip waste offcuts which I have tried to get to a point through the pugmill to be able to do wheelwork .</p>
<p>I have experimented with added Grogs and Kaolin.</p>
<p>The big problem with the clay, which has been prepared for pouring ,firstly by adding Darvan/ dispersant. Makes a Great slip though! ...is that the non -Newtonian thixotropic character of this clay, because of earlier dispersant added creates a shear factor on the wheel which twists under…</p>
<p>We have a lot of recycled white slip waste offcuts which I have tried to get to a point through the pugmill to be able to do wheelwork .</p>
<p>I have experimented with added Grogs and Kaolin.</p>
<p>The big problem with the clay, which has been prepared for pouring ,firstly by adding Darvan/ dispersant. Makes a Great slip though! ...is that the non -Newtonian thixotropic character of this clay, because of earlier dispersant added creates a shear factor on the wheel which twists under pressure and is very difficult to centre.</p>
<p>I need to add something chemical etc. to the clay to break the negative charges on the clay particles, to attract rather than disperse. NOTE: If I take an oblong ball of clay in 2 hands and wring slightly, there is a twist of about 2 centimeters before the clay stiffens. Release and you can do it again... the vibration of the wheel also collapses this thixotropically.</p>
<p>Perfect clay though for rolling out.!</p>
<p>Any help will be very welcome please.</p>