George Lewter's Discussions (470)

Discussions Replied To (229) Replies Latest Activity

"About 1/4 of the volume of your pots (or even less) should allow you to pour a liner…"

George Lewter replied Feb 3, 2018 to Glazing inside large pots

3 Aug 2, 2018
Reply by Ayjay

"I moved your picture inline of the article for graphic impact. If this is an issue I…"

George Lewter replied Dec 11, 2017 to I am teaching an online Ian Currie Grid Glaze course

3 Dec 12, 2017
Reply by John Post

"Back in 2012 when we did the peer group basic accounting class, Wave accounting did…"

George Lewter replied Apr 26, 2017 to Buisness Accounting, looking for info

4 Apr 26, 2017
Reply by George Lewter

"We tried wave accounting for our accounting group class several years ago. As I reca…"

George Lewter replied Apr 22, 2017 to Buisness Accounting, looking for info

4 Apr 26, 2017
Reply by George Lewter

"Get into the Way-Back machine, and take a look at Charan Sachar's video posted in 20…"

George Lewter replied Jan 24, 2017 to Slip trailing

9 Jan 24, 2017
Reply by Lawrence Weathers

"Tony Hansen at Digital Fire has an extensive article on rutile (and almost every oth…"

George Lewter replied Jan 22, 2017 to Light Rutile Substitute

11 Mar 7, 2017
Reply by Judith Stoudmann

"My main use is for the glaze Nutmeg. It formerly was a light tan breaking red brown…"

George Lewter replied Jan 11, 2017 to Light Rutile Substitute

11 Mar 7, 2017
Reply by Judith Stoudmann

Stars

"20 oz. HVLP Gravity Feed Air Spray Gun with Regulator Central Pneumatic - Item#6…"

George Lewter replied Aug 15, 2016 to Spraying glazes

56 Sep 11, 2016
Reply by Jim Wallace

"Tom, gotta say I admire your dedication in mixing both your own clay and glazes. I s…"

George Lewter replied Aug 13, 2016 to What a difference the choice of clay makes.

12 Aug 13, 2016
Reply by George Lewter

"Top end holds might accomplish what you want. If you fire to cone five and then hold…"

George Lewter replied Jun 22, 2016 to Firing to cone 6 twice in the same firing?

14 Jun 28, 2016
Reply by Pat

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service