Tom Anderson's Discussions (44)

Discussions Replied To (39) Replies Latest Activity

"George, it would be nearly impossible to replicate the differences between light and…"

Tom Anderson replied Jan 9, 2017 to Light Rutile Substitute

11 Mar 7, 2017
Reply by Judith Stoudmann

"That is certainly a justifiable and good reason to purchase 350 mesh. However, Imsil…"

Tom Anderson replied Nov 17, 2016 to Soda firing

8 Jan 2, 2017
Reply by Norm Stuart

"Norm: Have you ever experimented with using Minex 400 in lieu of 270? Particle/mesh…"

Tom Anderson replied Nov 17, 2016 to Soda firing

8 Jan 2, 2017
Reply by Norm Stuart

"Larry: The only time I have used it is when mixing magnesium and cobalt colorants. I…"

Tom Anderson replied Oct 24, 2016 to glaze flaking off in high magnesium glazes

6 Jan 12, 2017
Reply by Tom Anderson

"Norm: I think cobalt needs to be added to the acidic column: my cobalt crystalline g…"

Tom Anderson replied Oct 24, 2016 to Green Pooling Blue glaze

14 Nov 30, 2016
Reply by Tileworks

"hi Lawrence: Crystalline glaze is notorious for being more flaky than granny's' bisc…"

Tom Anderson replied Oct 24, 2016 to glaze flaking off in high magnesium glazes

6 Jan 12, 2017
Reply by Tom Anderson

"Norm: I have studied amphoretic oxides for years: not a lot of good information out…"

Tom Anderson replied Oct 23, 2016 to Green Pooling Blue glaze

14 Nov 30, 2016
Reply by Tileworks

"Daniel: Have you done any experimenting with high purity ingredients? Case in point:…"

Tom Anderson replied Aug 18, 2016 to Can one predict the appearance of a glaze? (part I: The Si/Al ratio)

9 Oct 19, 2016
Reply by Tom Humphries

"HI Daniel, pleasure to meet you sir. When I seen the thread topic "Si/Al" ratios, I…"

Tom Anderson replied Aug 17, 2016 to Can one predict the appearance of a glaze? (part I: The Si/Al ratio)

9 Oct 19, 2016
Reply by Tom Humphries

"Norm: Has anyone considered using kyanite in flameware? Likewise it produces elongat…"

Tom Anderson replied Aug 15, 2016 to Non plastic CLAY

6 Aug 16, 2016
Reply by Norm Stuart

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2024   Created by Andrea Wolf.   Powered by