Penny Berglund's Discussions (13)

Discussions Replied To (12) Replies Latest Activity

"I will try this next test go round. It would make sense with the large bubbles I got…"

Penny Berglund replied Aug 29, 2018 to John Britt's Snowflake Crackle - The cone 6 oxidation glazes

29 Feb 19, 2019
Reply by JC

"I contacted John Britt, and other than trying other clay bodies, he had no suggestio…"

Penny Berglund replied Aug 29, 2018 to John Britt's Snowflake Crackle - The cone 6 oxidation glazes

29 Feb 19, 2019
Reply by JC

"Thanks! I will keep testing. I will see what I can get in the broad area I call loca…"

Penny Berglund replied Jul 29, 2018 to John Britt's Snowflake Crackle - The cone 6 oxidation glazes

29 Feb 19, 2019
Reply by JC

"I will try another clay body. I will also ask my supplier what they think. I am gett…"

Penny Berglund replied Jul 29, 2018 to John Britt's Snowflake Crackle - The cone 6 oxidation glazes

29 Feb 19, 2019
Reply by JC

"I did a new test run with a much better bisque protocol and a glaze test firing. I a…"

Penny Berglund replied Jul 29, 2018 to John Britt's Snowflake Crackle - The cone 6 oxidation glazes

29 Feb 19, 2019
Reply by JC

"Tom, That is very interesting. It sounds like a great way to run a real test. I look…"

Penny Berglund replied Jul 11, 2018 to John Britt's Snowflake Crackle - The cone 6 oxidation glazes

29 Feb 19, 2019
Reply by JC

"I broke a couple of the plates/bowls to see what I might learn. I did not find any e…"

Penny Berglund replied Jul 11, 2018 to John Britt's Snowflake Crackle - The cone 6 oxidation glazes

29 Feb 19, 2019
Reply by JC

"I will test this as well. My friend Paul suggested Neph Sy might be the source as we…"

Penny Berglund replied Jul 11, 2018 to John Britt's Snowflake Crackle - The cone 6 oxidation glazes

29 Feb 19, 2019
Reply by JC

"I am pretty sure I did a poor bisque job on this batch. John Britt uses this on iron…"

Penny Berglund replied Jul 11, 2018 to John Britt's Snowflake Crackle - The cone 6 oxidation glazes

29 Feb 19, 2019
Reply by JC

"It is a dark brown clay body. I spoke with my supplier and I will modify my bisque s…"

Penny Berglund replied Jul 11, 2018 to John Britt's Snowflake Crackle - The cone 6 oxidation glazes

29 Feb 19, 2019
Reply by JC

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service