Jeff Poulter's Discussions (111)

Discussions Replied To (98) Replies Latest Activity

"Here are a couple of quotes from Terry Fallon from over on the Crystalline Glaze Fou…"

Jeff Poulter replied Aug 26, 2013 to Kiln Element Life

18 Mar 10, 2015
Reply by Jeff Poulter

"Hi Robert,     Which Skutt is it?  My little KM-818 will go to ^10.  It doesn't like…"

Jeff Poulter replied Aug 26, 2013 to Firing Schedule - Fine tuning your electric kiln controller

45 Aug 27, 2013
Reply by Norm Stuart

"One thing you might want to consider is going to SSR's for your kiln when your relay…"

Jeff Poulter replied Aug 26, 2013 to Kiln Element Life

18 Mar 10, 2015
Reply by Jeff Poulter

"Yes, the wire will have to match since you are changing the metals which supply the…"

Jeff Poulter replied Aug 26, 2013 to Firing Schedule - Fine tuning your electric kiln controller

45 Aug 27, 2013
Reply by Norm Stuart

"Type S is typically what is used.  I got mine direct from Bartlett.  I lied, it was…"

Jeff Poulter replied Aug 25, 2013 to Firing Schedule - Fine tuning your electric kiln controller

45 Aug 27, 2013
Reply by Norm Stuart

"Let me clarify.  I won't use a type k for anything but bisque.  Yes, you can put a p…"

Jeff Poulter replied Aug 25, 2013 to Firing Schedule - Fine tuning your electric kiln controller

45 Aug 27, 2013
Reply by Norm Stuart

"Also one thing I do quite often is to set greenware on top of the kiln before I star…"

Jeff Poulter replied Aug 25, 2013 to Something Exploded in the Kiln - Was It Clay fatigue?

13 Aug 26, 2013
Reply by Meredith Walker

"Had any of the shelves been exposed to water?  Shelves that have soaked up enough wa…"

Jeff Poulter replied Aug 25, 2013 to Something Exploded in the Kiln - Was It Clay fatigue?

13 Aug 26, 2013
Reply by Meredith Walker

"Type K's are down hill from the first firing.  The metal immediately starts to defor…"

Jeff Poulter replied Aug 22, 2013 to Firing Schedule - Fine tuning your electric kiln controller

45 Aug 27, 2013
Reply by Norm Stuart

"So Norm,     The Neph Sy is the culprit.  I was wondering 'cause there were some thi…"

Jeff Poulter replied Aug 19, 2013 to Glossy glaze coming out Matt

19 Aug 19, 2013
Reply by Norm Stuart

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2026   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service