Norm Stuart's Discussions (511)

Discussions Replied To (426) Replies Latest Activity

"Your Genesis controller communicates only with Bartlett's server via the WiFi card a…"

Norm Stuart replied Jan 23, 2018 to Kiln Controller Bartlett Genesis LT-3140

36 Feb 10, 2018
Reply by Joseph Fireborn

"I'd call Bartlett, 319-372-8366,  as they make all of these kiln controllers and the…"

Norm Stuart replied Jan 2, 2018 to Kiln Controller Bartlett Genesis LT-3140

36 Feb 10, 2018
Reply by Joseph Fireborn

"I know from experience it's very important to use a shielded lead wire with the lowe…"

Norm Stuart replied Nov 30, 2017 to Kiln Controller Bartlett Genesis LT-3140

36 Feb 10, 2018
Reply by Joseph Fireborn

"I'm glad to hear software version 3.18.9 solved your firing accuracy problems as it…"

Norm Stuart replied Nov 20, 2017 to Kiln Controller Bartlett Genesis LT-3140

36 Feb 10, 2018
Reply by Joseph Fireborn

"I assume beta version 3.18.9 solves the problem you're experiencing as it did for us…"

Norm Stuart replied Nov 17, 2017 to Kiln Controller Bartlett Genesis LT-3140

36 Feb 10, 2018
Reply by Joseph Fireborn

"A PID program working correctly varies the heat output constantly to keep the measur…"

Norm Stuart replied Nov 15, 2017 to Kiln Controller Bartlett Genesis LT-3140

36 Feb 10, 2018
Reply by Joseph Fireborn

"Light rutile is dark rutile which is already fired to eliminate off-gassing from com…"

Norm Stuart replied Oct 28, 2017 to Light or dark rutile

3 Nov 19, 2017
Reply by Richarde Talbot

"I'm really impressed with Dave Bartlett's improved temperature control with the new…"

Norm Stuart replied Oct 25, 2017 to Kiln Controller Bartlett Genesis LT-3140

36 Feb 10, 2018
Reply by Joseph Fireborn

"Stacy - I just uploaded the Alfred Education files to your MediaFire FileDrop. Post…"

Norm Stuart replied Oct 7, 2017 to Alfred University Fundamentals of Ceramics

13 May 3, 2021
Reply by cp dunbar

"One of the best things about the new Genesis Kiln Controller is being able to downlo…"

Norm Stuart replied Oct 7, 2017 to Kiln Controller Bartlett Genesis LT-3140

36 Feb 10, 2018
Reply by Joseph Fireborn

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2025   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service