Joseph Fireborn's Discussions (66)

Discussions Replied To (51) Replies Latest Activity

"My blog is JosephFireborn.com, you can go back through my 2 years of development if…"

Joseph Fireborn replied Jun 23, 2016 to Firing to cone 6 twice in the same firing?

14 Jun 28, 2016
Reply by Pat

" This is the final result. "

Joseph Fireborn replied Jun 23, 2016 to Firing to cone 6 twice in the same firing?

14 Jun 28, 2016
Reply by Pat

"I am going to setup a currie grid test for that exact reason down the line. Right no…"

Joseph Fireborn replied Jun 23, 2016 to Firing to cone 6 twice in the same firing?

14 Jun 28, 2016
Reply by Pat

"Results are in, the firing to cone 6 twice showed no real difference in glaze smooth…"

Joseph Fireborn replied Jun 23, 2016 to Firing to cone 6 twice in the same firing?

14 Jun 28, 2016
Reply by Pat

"Welp. I am firing the test right now. Currently going to cone 6 then dropping to 194…"

Joseph Fireborn replied Jun 22, 2016 to Firing to cone 6 twice in the same firing?

14 Jun 28, 2016
Reply by Pat

"My standard firing profile was cone 5 with a 60 minute hold to cone 6 (verified with…"

Joseph Fireborn replied Jun 22, 2016 to Firing to cone 6 twice in the same firing?

14 Jun 28, 2016
Reply by Pat

"Any synthetic will do I presume, I just know axners, its the only thing I order from…"

Joseph Fireborn replied Jun 6, 2016 to Mason stains, or what?

5 Jun 6, 2016
Reply by Joseph Fireborn

"I agree with the beginning firings being so limited, I bought a smaller kiln than I…"

Joseph Fireborn replied Jun 5, 2016 to Mason stains, or what?

5 Jun 6, 2016
Reply by Joseph Fireborn

"I can't tell from the picture since it is so zoomed in, but the second picture looks…"

Joseph Fireborn replied Jun 4, 2016 to Mason stains, or what?

5 Jun 6, 2016
Reply by Joseph Fireborn

"No problem, I figured you had, but you never know. Sometimes it's easy to miss thing…"

Joseph Fireborn replied Mar 11, 2016 to Copper reds in oxidation using silicon carbide

6 Mar 11, 2016
Reply by Joseph Fireborn

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014