"The glycerin is more of a humectant which attracts moisture. For chemicals I use Am…"

Norm Stuart replied Mar 12, 2018 to gum in glazes

8 Jan 25, 2019
Reply by Norm Stuart

"Bentonite, clay, calcium chloride and epsom salts all flocculate, making a glaze thi…"

Norm Stuart replied Mar 9, 2018 to gum in glazes

8 Jan 25, 2019
Reply by Norm Stuart

"Gum burns out while Bentonite and Clay do not. So the one glaze I add gum to is a "r…"

Norm Stuart replied Mar 8, 2018 to gum in glazes

8 Jan 25, 2019
Reply by Norm Stuart

"Like paper in paper clay, corn starch is made up of carbon, hydrogen and oxygen - al…"

Norm Stuart replied Mar 4, 2018 to Firing with Cornstarch on the Clay Surface

6 Mar 4, 2018
Reply by Barbara Hanselman

"Here's a sample of 12 glazes which have an interesting break in the Insight Live Gla…"

Norm Stuart replied Feb 26, 2018 to Glazes that break over images well

2 Feb 26, 2018
Reply by Norm Stuart

"Very nice. I can't wait to see it over time Our Cress E-23 has power to spare to th…"

Norm Stuart replied Feb 10, 2018 to Kiln Controller Bartlett Genesis LT-3140

36 Feb 10, 2018
Reply by Joseph Fireborn

"The controller saves the previous ten firing logs with two files in csv format. The…"

Norm Stuart replied Jan 24, 2018 to Kiln Controller Bartlett Genesis LT-3140

36 Feb 10, 2018
Reply by Joseph Fireborn

"Thanks for the heads-up Joseph. I signed up for a User ID and password on the Bartle…"

Norm Stuart replied Jan 24, 2018 to Kiln Controller Bartlett Genesis LT-3140

36 Feb 10, 2018
Reply by Joseph Fireborn

"Your Genesis controller communicates only with Bartlett's server via the WiFi card a…"

Norm Stuart replied Jan 23, 2018 to Kiln Controller Bartlett Genesis LT-3140

36 Feb 10, 2018
Reply by Joseph Fireborn

"I'd call Bartlett, 319-372-8366,  as they make all of these kiln controllers and the…"

Norm Stuart replied Jan 2, 2018 to Kiln Controller Bartlett Genesis LT-3140

36 Feb 10, 2018
Reply by Joseph Fireborn

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2025   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service