"Alberta Slip II is Ravenscrag Slip according to Tony Hansen.  I don't find too many…"

Norm Stuart replied Mar 27, 2014 to Alberta Slip II

2 Mar 28, 2014
Reply by Jeff Poulter

"Having made many spreadsheets over my career I can tell you that's a deluxe spreadsh…"

Norm Stuart replied Mar 27, 2014 to Orton: calculation spreadsheet

1 Mar 27, 2014
Reply by Norm Stuart

"Jan - Do you find any difference between Eckalite or Eckaglass?  They seem very simi…"

Norm Stuart replied Mar 26, 2014 to Dry Glazes, Slips, Terra Sigilatta and Engobes for Cone 6 - Recipes and Techniques

17 Jun 2, 2015
Reply by Norm Stuart

"I've found Calcium Chloride more effective and easier to use than Epsom Salts (Magne…"

Norm Stuart replied Mar 26, 2014 to Flocculating and deflocculating

22 Jun 17, 2019
Reply by Sharon Canfield

"Before widespread electric lighting, chickens stopped laying eggs during the darker…"

Norm Stuart replied Mar 24, 2014 to Magic Water for slip

6 Mar 24, 2014
Reply by Nadine Mercader

"When purchasing ceramic supplies, like Sodium Silicate also called Water Glass, the…"

Norm Stuart replied Mar 22, 2014 to Magic Water for slip

6 Mar 24, 2014
Reply by Nadine Mercader

"This version of Jen's Juicy Fruit with Spodumene relies on less lithium carbonate wh…"

Norm Stuart replied Mar 20, 2014 to Issues with Jen's Juicy Fruit - Only problem glaze in a full load of tests?????

11 Mar 24, 2014
Reply by Ayjay

"May I suggest Jen's Juicy Fruit - Revised.  I've never been happy with the original,…"

Norm Stuart replied Mar 20, 2014 to Issues with Jen's Juicy Fruit - Only problem glaze in a full load of tests?????

11 Mar 24, 2014
Reply by Ayjay

"Regarding the MOK-623 Frit Alisa Clausen used when making "Cassie's Marsala".  Cassi…"

Norm Stuart replied Mar 17, 2014 to Replacing Materials that Are No Longer Produced or Have Changed Greatly

9 Jun 9, 2016
Reply by Dani Montoya

"I have a substitute for Johnson Matthey Frit 623  aka (B33X7, MOK623) in the Insight…"

Norm Stuart replied Mar 17, 2014 to Replacing Materials that Are No Longer Produced or Have Changed Greatly

9 Jun 9, 2016
Reply by Dani Montoya

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2025   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service