Norm Stuart's Discussions (511)

Discussions Replied To (426) Replies Latest Activity

"$10 a month for Photoshop is certainly a lot more reasonable than purchasing the pro…"

Norm Stuart replied Apr 22, 2014 to Photographing Your Work

17 Feb 19, 2019
Reply by JC

"The only reasonable way to deal with Laguna Clay is to use their Axner website to ob…"

Norm Stuart replied Apr 18, 2014 to Talc versions at Aardvark

7 Aug 4, 2014
Reply by Darthe Hues

"When I do a Google search of C2773 I only get references to Aardvark's website, so t…"

Norm Stuart replied Apr 16, 2014 to Talc versions at Aardvark

7 Aug 4, 2014
Reply by Darthe Hues

"That's a pretty comprehensive presentation. I especially liked your choice of Doroth…"

Norm Stuart replied Apr 16, 2014 to Chemistry in Ceramics

2 Apr 16, 2014
Reply by Daniel Spruyt

"Do you have a download of Glazeval?  I've played a little with Glaze Simulator which…"

Norm Stuart replied Apr 16, 2014 to Keeping record of your work

2 Apr 16, 2014
Reply by Daniel Spruyt

"Crawl glazes with a high percentage of Light Magnesium Carbonate and engobes are the…"

Norm Stuart replied Apr 12, 2014 to how thick should your glaze be sprayed on and how do you tell if it is that thick?

13 Apr 14, 2014
Reply by Jennifer Arthur

"Test tiles are the only answer.  Listed in the Insight Database as Heidi's Eggshell,…"

Norm Stuart replied Apr 12, 2014 to how thick should your glaze be sprayed on and how do you tell if it is that thick?

13 Apr 14, 2014
Reply by Jennifer Arthur

"This is Frogskin on porcelain fired to ^6 with a very slow-cool from 1,800 F to 1,50…"

Norm Stuart replied Apr 11, 2014 to PA Frogskin Glaze

22 Apr 11, 2014
Reply by Norm Stuart

"Remember that you can easily fix over-flocculation with a deflocculant, or the rever…"

Norm Stuart replied Apr 9, 2014 to Flocculating and deflocculating

22 Jun 17, 2019
Reply by Sharon Canfield

"Simply lower the flint from 16.5 to 15.75, add 0.5 silicon carbide and see what happ…"

Norm Stuart replied Apr 2, 2014 to silicon carbide in red reduction glazes for an oxidation environment?

12 Jul 7, 2014
Reply by Jeff Poulter

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2025   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service