George Lewter's Discussions (470)

Discussions Replied To (229) Replies Latest Activity

"Links for spraying information and equipment available in the US. Here is a good gen…"

George Lewter replied Jun 3, 2011 to Spraying glazes

56 Sep 11, 2016
Reply by Jim Wallace

"I tested the Matte Black recipe last week and was quite pleased with the results.  B…"

George Lewter replied May 7, 2011 to Recipes for Testing

6 Oct 30, 2013
Reply by George Lewter

"A picture of a piece by Catherine Rehbein, "Rippled Waters", prompted a comment by P…"

George Lewter replied May 1, 2011 to The Best of Cone 6, Mid-Fire Potters

22 Dec 10, 2012
Reply by George Lewter

"Here is  Brian Gartside's Webpage on his base glaze and variations and his more deta…"

George Lewter replied Apr 22, 2011 to Gartside Base

3 Dec 3, 2011
Reply by Tess van Dijk

"ADDING IMAGES TO YOUR POSTINGS AND COMMENTS To place a picture in a comment or other…"

George Lewter replied Apr 21, 2011 to Network User Guide and General Info to Improve Member Interactions

8 Jan 22, 2015
Reply by Corina

"Laurie Niswander's Sea turtle jar keeps popping up in the slide show.  I just realiz…"

George Lewter replied Apr 19, 2011 to The Best of Cone 6, Mid-Fire Potters

22 Dec 10, 2012
Reply by George Lewter

"Go to Anthony's profile page, scroll down to the slideshow, and click the "View All"…"

George Lewter replied Apr 19, 2011 to The Best of Cone 6, Mid-Fire Potters

22 Dec 10, 2012
Reply by George Lewter

"I heartily agree, Anthony's photos are "Da Bomb"!"

George Lewter replied Apr 19, 2011 to The Best of Cone 6, Mid-Fire Potters

22 Dec 10, 2012
Reply by George Lewter

"For glaze spraying, gravity fed hvlp guns have a definite advantage. Glaze is being…"

George Lewter replied Apr 16, 2011 to Spraying glazes

56 Sep 11, 2016
Reply by Jim Wallace

"One thing about dry mixes is there can be some differential settling or incomplete m…"

George Lewter replied Apr 14, 2011 to Glaze Cracks and Flakes Off Before Firing

6 Apr 14, 2011
Reply by Ceci

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2025   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service