Norm Stuart's Discussions (511)

Discussions Replied To (426) Replies Latest Activity

"The glaze with the added iron oxide is very nice. What percentage copper carbonate d…"

Norm Stuart replied Jun 1, 2015 to Assad Black

12 Jun 1, 2015
Reply by Gina Skillings

"Once the temperature rises to just 554 F (290 C) Copper Carbonate (Cu2 (OH)2 CO3) qu…"

Norm Stuart replied May 30, 2015 to Assad Black

12 Jun 1, 2015
Reply by Gina Skillings

"This is Digitalfire's commentary on Copper Oxide, which is a black matte powder. ht…"

Norm Stuart replied May 30, 2015 to Assad Black

12 Jun 1, 2015
Reply by Gina Skillings

"It's obvious the "Mocha Staining" created by Tony Remington, the potter in the video…"

Norm Stuart replied May 11, 2015 to Mocha Diffusoin

18 Aug 17
Reply by tony remington

"If you are looking at novel materials, do this Google search for decomposition tempe…"

Norm Stuart replied May 9, 2015 to Copper Sulphate - what' it good for?

4 May 15, 2015
Reply by Marina Reijsmeijer (Kleierij)

"The percentage of Mason Stain varies by color to achieve the same intensity. As much…"

Norm Stuart replied May 9, 2015 to Clear Glaze for Mason Stains

9 May 9, 2015
Reply by Norm Stuart

"I haven't had a high success rate with repair firings. Cracks usually seem to get la…"

Norm Stuart replied Apr 28, 2015 to Post firing/glazing repairs

7 Jun 11, 2015
Reply by Marla Stroup

"Glaze applied thick all at once can definitely peel off the bisque as it dries, ulti…"

Norm Stuart replied Apr 25, 2015 to Cone 6 tests with Digital Fire Bases

6 Apr 25, 2015
Reply by Norm Stuart

"Many potters in England prefer to call SiO2 Flint while most Americans call it Silic…"

Norm Stuart replied Apr 24, 2015 to Cone 6 tests with Digital Fire Bases

6 Apr 25, 2015
Reply by Norm Stuart

"There's a limitation to the effectiveness in removing salts from clay by pouring-off…"

Norm Stuart replied Apr 23, 2015 to Frozen Clay??

10 Apr 27, 2015
Reply by Barbara Howe

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2025   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service