ceramic supply usa - liston crystalline glazes

So about the same time that Coyote came out with their non-running crystalline glazes, my buddy(Clay Liston) who works for Ceramic Supply U…

Started by Jeff Poulter

1 Jun 10, 2014
Reply by Nadine Mercader

How to interpret this recipe for Lynn's Glossy Gray-blue green

I am trying to mix the recipe that is the glaze on Barbara Hanselman's  'Egyptian Bowl'. Gerstly borate     50 Silica                   3…

Started by martha peddicord

1 Apr 19, 2014
Reply by Wyndham Dennison

Keeping record of your work

OK, I give it another try...Integrated in my database mentioned before, I developed a system to evaluate glazes and it can - to some extend…

Started by Daniel Spruyt

2 Apr 16, 2014
Reply by Daniel Spruyt

Keeping record of your work

If you use many different glazes or always try new ones like me, it is important to keep record of everything you do. To do so I use the re…

Started by Daniel Spruyt

0 Apr 13, 2014

Refire Test Ring from previous Cone 6 Test to 1000c and Intereting Results

Recently I opened a discussion here with my first test cone 6 test results and photos. I explained that due to circumstances, I did not do…

Started by Jan Wallace

9 Feb 25, 2014
Reply by Norm Stuart

Recipes for Testing

If you find a recipe that intrigues you and want to know more about it, post it here to see if anyone else has any experience with it.  Ple…

Started by George Lewter

6 Oct 30, 2013
Reply by George Lewter

Glaze tests

There are a number of glaze tests on my web site in the Potters Corner if anyone is interested.  Many tiles are layered glazes some of whic…

Started by Randy McCall

18 Jul 25, 2013
Reply by Judy Smith

Online Glaze Recipe Database Project is Now Under Way

Tony Hansen, owner of the Digitalfire Corporation contacted me after my  announcement went out that we were about to develop an online glaz…

Started by George Lewter

15 Jan 20, 2013
Reply by June Perry

The Accidental Glaze Project

The Accidental Glaze Project “Name the greatest of all inventors. Accident.” Mark Twain Has this happened to you? Out of the kiln comes a n…

Started by Tobla Howell

0 Dec 10, 2012

CORRECTED LIST AND NEW PHOTO OF CONE 6 TESTS

  The first four glazes in the front row (left to right), which were on the top shelf of the kiln, are my SCM version #10812A with 2% yell…

Started by June Perry

5 Apr 14, 2012
Reply by Darthe Hues

RSS

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2022   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service