Has anyone previously used Laguna WC-391 B-3 Brown Clay?

We bought one box to try out and the first person to use this clay made a slab construction of  about 3/8 inches thick.

This clay bloated in a Cone 6 firing, due to some part of the clay that is off-gassing.  The ware was previously bisque fired to Cone 04 and had a thin layer of clear glaze on it.

http://www.lagunaclay.com/clays/western/wc391.php

This clay is listed by Laguna as Cone 5, but I've never seen this problem in a Cone 5 clay fired to Cone 6.

Views: 1905

Comment

You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!

Join Electric Mid&Hi Fired Ceramics

Comment by Norm Stuart on August 4, 2014 at 6:37pm

You'd certainly hope a slow bisque to cure many problems later.

But many clays bloat, melt or experience other defects when fired hotter than their temperature range as the components of the clay decompose at these temperatures much hotter than bisque.. 

Unfortunately some batches of clay will also bloat when fired under their maximum temperature range due to raw material additions which don't meet specifications.

Comment by Darthe Hues on August 4, 2014 at 1:34pm

I watched this video on YouTube: http://youtu.be/tq7TdWkICZ0

The teacher said that doing a very slow bisque firing to higher temperature would take care of a lot of flaws that would come later in the glaze firing like pinholing, etc. because it allows more time for the gases to work their way to the surface. Especially with thicker pieces.

Comment by Norm Stuart on February 28, 2014 at 8:02am

Thanks.  I'll try some WC-391 tiles myself when the rains stop.  I'll see if the bloating is from the thickness of his slabs or the Cone 6 firing.  It's not something I'd expect when bisquing to cone 04 with a 20 minute hold.

Comment by Robert Coyle on February 28, 2014 at 7:56am

Just did some thin test tiles (1/4") . Looked OK but only fired to cone 5. Glazes seemed to strike in more than usual.

Videos

  • Add Videos
  • View All

Use These Links to Support Us

Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase 

Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com

Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.comMastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.

Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.

The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.

Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .

If you are up to creating videos of your work or techniques you might want to invest in a flip video camera

Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00

And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62

ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.

Tips for Members

If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014

© 2025   Created by Andrea Wolf.   Powered by

Badges  |  Report an Issue  |  Terms of Service