Recipe is from Fat Cat Pottery, the coop studio where I have been working for last 4 years
1000 grams
Wollastonite 100
Frit 3134 350
EPK 150
Silica 150
Custer Feldspar 250
add Zircopax 200
Do you mind sharing your glossy white base? I've been testing on-glaze/majolica combos of late. It's been surprisingly challenging.
Yes, yes. What Fireborn said. Looking forward to seeing vertical surfaces!
No way! Don't try to prevent them! They are stunning. I can't wait to see the vertical surface. Very nice work sir.
They are in the wash. red iron oxide mixed with water 3 to 1 ration by volume makes the wash too runny so I added gum solution to thicken the mixture which made it more controlled when brushing ( I use it on vertical surfaces also - cups and vases) (will post a close up of the cup surface tomorrow) The mixing action creates small bubbles in the wash which transfer to the piece, but I kind of like them so have not tried to prevent them, Thanks for the encouragement.
The spots in the iron wash, are those due to the trails or is that some kind of spotting from the wash? They are very interesting. This tray is fantastico!
Low cost flat lapping disc can be used on you potters wheel if you, drill bat pin holes in it, and provide a trickle of water to cool it. At amazon.com, 120 grit for aggressive material removal. Click the image to purchase
Members have had great things to say about John Britt's new book, Mid-Range Glazes. Click the image to buy from Amazon.com
Purchase Glazes Cone 6 by Michael Bailey, The Potters Book of Glaze Recipes by Emmanuel Cooper, or Making Marks by Robin Hopper, all available at amazon.com. Mastering Cone 6 Glazes by John Hesselberth & Ron Roy is now out of print.
Harbor Freight is a great place to find unbeatable prices for better HVLP spray guns with stainless steel parts and serviceable economy models, as well as detail guns, all tested by our members for spraying glazes, as well as compressors to power the guns. As yet no one has tested and commented on the remarkably inexpensive air brushes at harbor freight.
The critter siphon gun is a spray alternative that is well liked by some of our members, and is available at amazon.
Amazon is also a competitive source for photo light tents for shooting professional quality pictures of your work. They also have the EZ Cube brand favored by several of our members. You might also want to purchase the book Photographing Arts, Crafts and Collectibles . . .
If you are up to creating videos of your work or techniques you might want to invest in a flip video camera
Following are a few scales useful for potters. Ohaus Triple Pro Mechanical Triple Beam Balance, 2610g x 0.1g, with Tare $169.00
And finally a low cost clone of the OHaus. The Adam Equipment TBB2610T Triple Beam Mechanical Balance With Tare Beam $99.62
ebay is a great alternative for many tools and the equipment used in the ceramics studio - kilns, wheels, extruders, slab rollers are often listed there both new and used.
If you just want to spout off, it is best accomplished as a blog posting. If you want to get more guidance and ideas from other members, ask a question as a new discussion topic. In the upper right corner of the lists for both types of posting, you will find an "+Add " button. Clicking it will open an editor where you create your posting. 4/16/2014
© 2024 Created by Andrea Wolf. Powered by
You need to be a member of Electric Mid&Hi Fired Ceramics to add comments!
Join Electric Mid&Hi Fired Ceramics